BOSTIK 70-01A

Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.

BOSTIK 70-01A

Main features

  • Permanently Elastic SMP Sealant with Temperature Resistance
  • Primerless Glass-to-Metal Bonding
  • Solvent-, Isocyanate-, and PVC-Free Formulation

Product Description

Bostik Simson ISR 70-01 is a one-component, moisture-curing sealant based on silyl-modified polymer technology. It forms a permanently elastic seal for industrial joints where movement, sound, or vibration must be accommodated. The solvent-, isocyanate-, and PVC-free formulation provides excellent UV and weather resistance, adheres to many clean substrates without primer, and remains elastic from -40°C to 100°C. It is paint-compatible with most industrial alkyd- and dispersion-based coating systems, subject to compatibility testing.

Key features

  • Permanent elasticity: Remains elastic across a service-temperature range of -40°C to 100°C.
  • Primerless adhesion on many substrates: Adheres to aluminum, stainless steel, galvanized steel, glass, PVC, polyester, and many coated surfaces when properly prepared.
  • Industrial processing flexibility: Provides approximately 30 minutes of skin-forming and tooling time at 20°C and 50% relative humidity and can be painted after skin formation.

Applications / Suitable for

  • Bus, caravan, train, and truck construction
  • Air-conditioning equipment
  • Aluminum airfreight containers
  • Sound- and vibration-reducing sealing applications

Bostik Simson ISR 70-01 is a one-component, moisture-curing sealant based on silyl-modified polymer technology. It forms a permanently elastic seal for industrial joints where movement, sound, or vibration must be accommodated. The solvent-, isocyanate-, and PVC-free formulation provides excellent UV and weather resistance, adheres to many clean substrates without primer, and remains elastic from -40°C to 100°C. It is paint-compatible with most industrial alkyd- and dispersion-based coating systems, subject to compatibility testing.

Key features

  • Permanent elasticity: Remains elastic across a service-temperature range of -40°C to 100°C.
  • Primerless adhesion on many substrates: Adheres to aluminum, stainless steel, galvanized steel, glass, PVC, polyester, and many coated surfaces when properly prepared.
  • Industrial processing flexibility: Provides approximately 30 minutes of skin-forming and tooling time at 20°C and 50% relative humidity and can be painted after skin formation.

Applications / Suitable for

  • Bus, caravan, train, and truck construction
  • Air-conditioning equipment
  • Aluminum airfreight containers
  • Sound- and vibration-reducing sealing applications

Technical Specifications

General Properties
Process Method
Moisture curing
Product Type
Material category or functional product class.
SMP adhesive & sealant
Thermal Properties
Operating Temperature
-40°C to +120°C °C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical product, application, and storage properties for Bostik Simson ISR 70-01.

Property Value Unit Method or condition
Basic material Silyl Modified Polymer — SMP technology
Curing method Moisture cure — One-component sealant
Specific gravity Approx. 1.4 g/mL Typical value
Skin-forming time Approx. 30 minutes 20°C and 50% RH
Curing speed after 24 hours Approx. 3 mm 20°C and 50% RH
Green strength Approx. 300 Pa Physica Rheometer MC100; maximum uncured load without sagging
Application temperature 5 to 35 °C Hand- or air-pressure gun application
Solvent content 0 % Typical product composition
Isocyanate content 0 % Typical product composition
Storage stability 12; cartridges 18 months Original unopened container, dry storage at 5°C to 30°C
Technical properties

After-processing / final-state properties

Typical cured and in-service properties for Bostik Simson ISR 70-01.

Property Value Unit Method or condition
Shore A hardness Approx. 26 Shore A DIN 53505
Volume change Less than 3 % DIN 52451
Tensile stress at 100% elongation Approx. 0.9 MPa DIN 53504 / ISO 37
Tensile stress at break Approx. 1.7 MPa DIN 53504 / ISO 37
Elongation at break Approx. 300 % DIN 53504 / ISO 37
Shear stress Approx. 1.8 MPa DIN 53283 / ASTM D1002; aluminum-to-aluminum, 2 mm adhesive thickness, 50 mm/min
Tear propagation Approx. 15 N/mm DIN 53515 / ISO 34; Type C, 500 mm/min
Temperature resistance -40 to 100 °C Cured product
UV and weather resistance Excellent — Supplier classification