BOSTIK 6363

Harmonization Code : 8473.30.80.00 | Parts and accessories (other than covers, carrying cases and the like) suitable for use solely or principally with machines of headings 8470 to 8472 ; Parts and accessories of the machines of heading 8471 ; Other; Other

BOSTIK 6363

Main features

  • Wide-Range Hot-Melt Viscosity Control
  • High-Temperature Service Range to 204 deg C
  • Standard 0.5 in Glue-Gun Stick Format

Product Description

Bostik Thermogrip 6363 Hot Melt Adhesive is a one-part, medium-setting, general-purpose ethylene vinyl acetate (EVA) hot-melt adhesive supplied in off-white 0.5 in x 15 in sticks. It cures by cooling at room temperature after application and is typically used for furniture repair and assembly, leather products, component staking on PC boards, and automotive assembly or repair. The adhesive has a service temperature of 176.7 to 204.4 deg C and a flash point above 204.4 deg C, with Brookfield viscosity decreasing from about 33,500 cP at 162.8 deg C to about 8,875 cP at 204.4 deg C as application temperature increases. It is supplied in 25 lb cases of sticks for use with compatible hot-melt glue guns or applicators.

Key features

  • EVA Hot-Melt Chemistry: one-part ethylene vinyl acetate hot-melt adhesive that cures by cooling at room temperature
  • Application Viscosity Range: viscosity decreases from about 33,500 cP at 162.8 deg C to about 8,875 cP at 204.4 deg C
  • 0.5 in x 15 in Glue-Gun Sticks: supplied in off-white sticks sized for standard hot-melt glue guns and applicators

Applications

Furniture repair and assembly, leather products, component staking on PC boards, and automotive assembly or repair.

Technical Specifications

General Properties
Density (g)
0.96 g/cm3
Thermal Properties
Operating Temperature
176.7 - 204.4 °C
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
see additional info section mPa.s

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
ColorOff-white-As supplied
Chemical compositionEVA (ethylene vinyl acetate)-As supplied
Cure systemRoom temperature-Cooling after application
Flash pointgreater than 204.4deg CAs reported
Service temperature176.7 to 204.4deg CApplication / service range
Viscosity33,500 to 8,875cPBrookfield, 162.8 to 204.4 deg C, decreasing with temperature

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers