BONDERITE S-FN 333

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

BONDERITE S-FN 333

Main features

Product Description

BONDERITE® S-FN 333 ACHESON is a resin-bonded dry film lubricant that combines fluorocarbon lubricants with a thermosetting resin to deliver a durable, low-friction coating for demanding industrial applications. Developed for applications beyond conventional fluorocarbon coatings, it provides excellent wear resistance, chemical resistance, and repairability while maintaining low friction and long service life on a wide variety of components. :contentReference[oaicite:0]{index=0}

Key Features

  • Fluorocarbon-based resin-bonded dry film lubricant for demanding wear applications.
  • Low coefficient of friction combined with excellent durability and wear resistance.
  • Excellent resistance to many acids, bases, solvents, and salt environments.
  • Repairable coating that can be overcoated without removing the original film.
  • Suitable for spray application on a wide range of metal components.

Applications / Suitable for

  • Business machine parts
  • Valve plugs and valves
  • Drawer guides
  • Window guides
  • Lock assemblies
  • Springs
  • Industrial tools
  • Filter systems
  • Printing equipment
  • Aerospace parts
  • Marine equipment
  • Rails, slides and chutes
  • Closed automotive assemblies

Technical Specifications

General Properties
Product Type
Material category or functional product class.
Resin-bonded fluorocarbon lubricant

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Method / Condition
Technology Dry film lubricant — Supplier classification
Pigment Blend of fluorocarbons — Wet product
Binder Thermoset — Wet product
Carrier BONDERITE L-FG SB-3 ACHESON — Wet product
Diluent BONDERITE L-FG SB-3 ACHESON — Wet product
Appearance Black liquid — Wet product
Viscosity 120–150 mPa·s Typical
Density 1.13 kg/L Typical
Solids content ~28 % by weight Typical
Flash point 57 °C Typical
VOC 808 g/L Typical
Recommended storage 24°C (75°F) — Original sealed container
Shelf life 2 years — Original sealed container
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Method / Condition
Coating color Black — Cured coating
Coefficient of friction 0.09–0.10 — Static and kinetic
Recommended dry film thickness 25.4 µm 0.001 in optimum thickness
Theoretical coverage 6.54 m²/kg @ 25 µm dry film thickness
Continuous service temperature 204–232 °C 400–450°F
Salt spray resistance >500 hours Over zinc phosphated surface, 25 µm film
Hartman Wear Test 200,000 cycles 180 lb load
Taber Abrasion Test 16.9 mg weight loss 1000 cycles
Chemical resistance Excellent resistance to selected acids, bases, sodium chloride solutions, ketones and aliphatic solvents — Cured coating
Typical cure cycle Preheat 149°C for 10 min, then cure at 260°C/15 min, 288°C/9 min, 316°C/5 min, 371°C/1 min, or 399°C/0.5 min — Substrate temperature