BONDERITE S-FN 330

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

BONDERITE S-FN 330

Main features

  • Low-Friction Stick-Slip-Resistant Coating
  • 500-Hour Salt-Spray/Humidity Resistance
  • Up to 150 deg C Service

Product Description

BONDERITE® S-FN 330 ACHESON is a resin-bonded dry film lubricant formulated with a fluorocarbon dispersion in a thermosetting binder for long-lasting, low-friction performance on metal components. Designed for spray application, it produces a durable coating that eliminates stick-slip behavior while improving wear resistance, corrosion protection, and service life in industrial and consumer applications. :contentReference[oaicite:0]{index=0}

Key Features

  • Resin-bonded fluorocarbon dry film lubricant for permanent low-friction coatings.
  • Produces low-friction coatings free of stick-slip characteristics.
  • Provides excellent corrosion and humidity resistance after curing.
  • Designed for spray application with one-package convenience.
  • Suitable for metal substrates in industrial and consumer applications.

Applications / Suitable for

  • Fasteners
  • Carburettor parts
  • Lock mechanisms
  • Water, gas and oil valves
  • Gears
  • Bearings

Technical Specifications

General Properties
Product Type
Material category or functional product class.
Fluorocarbon dry-film lubricant

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Method / Condition
Technology Lubricant — Supplier classification
Product type Fluorocarbon dispersion in solvent — Supplier description
Application Dry film lubricant — Supplier classification
Lubricant Fluorocarbon — Wet product
Binder Thermosetting resin — Wet product
Solids content 25–26 % Wet product
Viscosity (Brookfield) 60–150 mPa·s Wet product
Density ~960 kg/m³ Wet product
Flash point (open cup) 10 °C Wet product
Color Blue — Wet product
Recommended storage temperature 5–30 °C Unopened container
Shelf life 24 months Unopened original packaging
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Method / Condition
Recommended dry film thickness 10–25 µm Typical application
Theoretical coverage ~22 m²/kg @ 10 µm dry coating thickness
Coating color Green — Cured coating
Coefficient of friction (static & kinetic) 0.7 — Cured coating
Flexibility No loss of adhesion — 3.2 mm radius bend on 0.8 mm steel panels
Salt spray resistance >500 hours ASTM B117*
Humidity resistance >500 hours 98% RH at 49°C*
Continuous service temperature 150 °C Cured coating
Intermittent service temperature 160 °C Cured coating
Curing schedule 160°C / 60 min
180°C / 30 min
200°C / 10 min
— Substrate temperature

*Performance values based on coating cured at 160°C for 60 minutes on zinc phosphated steel with 0.025 mm coating thickness.

Leading Brands Trust in Our Products and Services