BONDERITE M-CR 1132 AERO TOUCH-N-PREP PEN

Harmonization Code : 3824.99.92.97 | Prepared binders for foundry molds or cores; chemical products and preparations of the chemical or allied industries (including those consisting of mixtures of natural products), not elsewhere specified or included: other : other : other

BONDERITE M-CR 1132 AERO TOUCH-N-PREP PEN

Main features

  • Ready-to-Use Touch-N-Prep Pen
  • No-Rinse Dry-in-Place Processing
  • Modifiable Felt-Tip Applicator

Product Description

BONDERITE® M-CR 1132 AERO Touch-N-Prep® Pen is a ready-to-use hexavalent chromium conversion coating applicator for localized touch-up and repair of aluminum and aluminum-alloy surfaces. The dry-in-place treatment is applied directly from the pen without rinsing and may be air-dried or force-dried with warm air. Its controlled felt-tip delivery system supports treatment of edges, holes, rivets, and other small or difficult-to-reach areas while reducing chemical use, worker contact with chromating solutions, and rinse-water waste compared with conventional chromating processes.

Key Features

  • Ready-to-use conversion coating: Delivers a dry-in-place hexavalent chromium treatment directly from the applicator pen without mixing or dilution.
  • No-rinse application: The applied coating can be air-dried or force-dried with warm air at a maximum recommended temperature of 60°C (140°F).
  • Controlled touch-up delivery: The felt-tip applicator supports localized treatment of edges, holes, rivets, and other small or difficult-to-reach aluminum surfaces.

Applications / Suitable for

  • Touch-up and repair of conversion coatings on aluminum and aluminum-alloy surfaces
  • Localized treatment of bare areas on aircraft and aircraft-part surfaces
  • Treatment of edges, rivets, holes, and other small or difficult-to-reach areas

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Felt-tipped type marker / Colorless

Additional Information

Technical Properties

After-Processing / Final-State Properties

Typical coating-weight and coverage guidance when two coats are applied.

Property Value Unit Method / Condition
Light Coating Weight 13 to 18 mg/ft² Class 1A and Class 3; two coats; approximately 50 ft² coverage per pen
Moderate Coating Weight 18 to 22 mg/ft² Class 1A and Class 3; two coats; approximately 35 ft² coverage per pen
Heavy Coating Weight 22 to 35 mg/ft² Class 1A only; two coats; approximately 25 ft² coverage per pen
Minimum Double-Coat Weight At least 10 mg/ft² When the applicator pen adequately wets the surface

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers