BONDERITE® L-FM PRETREAT AERO is a liquid lubricant and protective coating formulated to inhibit the formation of tenacious scale during heat treatment of ferrous metals, stainless steels, nickel-chromium alloys, and copper alloys in non-inert gas atmosphere furnaces. It also functions as a lubricant for hot forming and hot flaring of titanium, cold forming of 17-7 PH steel, a protective coating for carbon steel dies during hot sizing, a rust preventive for mild steel, and a protective coating for copper alloys during annealing. The coating significantly reduces metal loss, intergranular oxidation, and surface notching while minimizing the need for aggressive acid descaling after heat treatment. :contentReference[oaicite:0]{index=0}

Key Features

  • Inhibits tenacious scale formation during heat treatment of multiple metal alloys.
  • Reduces metal loss, intergranular oxidation, and surface notching.
  • Functions as both a forming lubricant and protective coating for hot and cold forming operations.
  • Shortens post-heat-treatment descaling time while minimizing the need for aggressive acid cleaning.
  • Spray-applied coating that dries rapidly and resists scuffing and fingerprinting.

Applications / Suitable for

  • Heat treatment of ferrous metals
  • Stainless steels
  • Nickel-chromium alloys
  • Copper alloys
  • Hot forming of sheet titanium
  • Hot flaring of titanium tubing
  • Cold forming of 17-7 PH steel plate
  • Carbon steel hot sizing dies
  • Rust prevention for mild steel
  • Protective coating during copper alloy annealing

Technical Specifications

General Properties
Product Type
Material category or functional product class.
Heat-treatment protective coating & forming lubricant
Thermal Properties
Operating Temperature
Dries at ambient; furnace processing in oxidizing atmosphere °C

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Method / Condition
Technology Lubricant forming / Protective coating — Supplier classification
Appearance Orange-colored liquid — As supplied
VOC 813 g/L Supplier value
Flash point 5 °C Tag Closed Cup
Storage temperature 0–40 °C Closed containers
Shelf life Not stated — Technical Process Bulletin
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Method / Condition
Recommended coating thickness 0.2–0.3 mil Maximum coating thickness
Drying time 1–5 minutes Normal atmospheric conditions
Film condition Light orange-gold coating resistant to scuffing and fingerprinting — After drying
Application method Spray (preferred) — Brush or adjusted spray viscosity as required
Spray pressure 35 psi Binks Model #7 with #36 SD tip (typical)
Furnace atmosphere Slightly oxidizing — Required for proper coating performance