BONDERITE C-IC ALDOX

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

BONDERITE C-IC ALDOX

Main features

  • Chromate-Free Aluminum Deoxidizing and Desmutting
  • Boeing BAC 5765 Qualification
  • Ambient Spray or Immersion Processing

Product Description

TURCO® ALDOX V (also known as BONDERITE C-IC ALDOX) is a dark brown, chromate-free liquid formulated to deoxidize, desmut, and lightly etch aluminum alloys. It is ideal for preparing alloys that require low surface resistance prior to anodizing, conversion coating, bonding, or welding.

Key features

  • Aerospace approved: Meets stringent Boeing BAC 5765 specifications for aerospace surface preparation.
  • Chromate-free formulation: Safely deoxidizes and desmuts without the use of chromates while remaining readily soluble in water.
  • Adjustable and versatile: Effective at ambient temperatures in both spray and immersion systems, with easily adjustable etch rates to meet specific requirements.

Applications / Suitable for

  • Deoxidizing, desmutting, and lightly etching aluminum alloys.
  • Surface preparation prior to anodizing, conversion coating, bonding, or welding.
  • Spray and immersion processing systems.

Technical Specifications

General Properties
Functionality
Acid cleaner, brightener, and pre-paint conditioner
Thermal Properties
Operating Temperature
15°C to 66°C (60°F to 150°F) °C

Additional Information

Technical properties

As-supplied / before-processing properties

Physical characteristics and operating parameters for TURCO® ALDOX V.

Property Value Unit Method / condition
Appearance Dark brown liquid - -
Operating Temperature 10 to 50 °C Optimum temperature is about 25°C
Concentration (TURCO ALDOX V) 15 (13 to 17) % by volume Final solution volume
Concentration (Nitric Acid) 25 (23 to 27) % by volume 42° Baumé Nitric Acid equivalent, final solution volume
Application Method Spray or Immersion - Operate spray system at 20 to 31 psi