BONDERITE C-IC 4409

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

BONDERITE C-IC 4409

Main features

  • Ferrous/Nonferrous Alloy Cleaning and Deoxidizing
  • Hand-Wipe, Immersion, or Spray Processing
  • Water/Steam-Rinsable Rust Removal

Product Description

BONDERITE® C-IC 4409 AERO is a liquid acid cleaner and deoxidizer formulated for cleaning and deoxidizing ferrous and nonferrous alloys by immersion, spray, or hand wipe application. The phosphoric acid-based formulation readily rinses with water or steam, imparts a satin finish on aluminum alloys, provides an excellent base for paint adhesion, and effectively removes rust from ferrous alloys. It is intended for use on a wide range of metals, but should not be used on magnesium alloys or high-strength steels. :contentReference[oaicite:0]{index=0}

Key Features

  • Liquid acid cleaner and deoxidizer for ferrous and nonferrous alloys.
  • Suitable for immersion, spray, and hand wipe application.
  • Produces a satin finish on aluminum while creating an excellent paint base.
  • Readily rinses with water or steam for efficient processing.
  • Effectively removes rust from ferrous alloys.

Applications / Suitable for

  • Aluminum alloys
  • Ferrous alloys
  • Nonferrous alloys
  • Paint surface preparation
  • Rust removal
  • General metal cleaning and deoxidizing

Technical Specifications

General Properties
Product Type
Material category or functional product class.
Acid cleaner & deoxidizer
Thermal Properties
Operating Temperature
Up to 140°F (60°C) °C

Additional Information

 
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Method / Condition
Surface finish Satin finish on aluminum alloys — After treatment
Paint preparation Produces an excellent base for paint — Aluminum alloys
Rust removal Removes rust from ferrous alloys — After treatment
Ambient immersion time 3–10 minutes 25–50% solution
Hot tank immersion time 3–10 minutes 5–10% solution
Maximum operating temperature 60 °C Immersion or spray
Application methods Hand wipe, immersion, spray — Mechanical agitation recommended