BONDERITE C-IC 33

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

BONDERITE C-IC 33

Main features

  • Non-Flammable Bonding Formulation
  • Brush, Spray, or Immersion Application
  • Adhesion-Promoting Surface Treatment

Product Description

BONDERITE® C-IC 33 AERO is a non-flammable phosphoric acid-based cleaner, brightener, and prepaint conditioner for aluminum. It removes oxidation and corrosion to produce a chemically clean, corrosion-free surface prior to welding, painting, or chemical conversion coating. The product is suitable for brush, immersion, and spray application, providing an effective surface preparation step for improved coating adhesion and corrosion resistance. :contentReference[oaicite:0]{index=0}

Key Features

  • Non-flammable phosphoric acid-based formulation for cleaning and conditioning aluminum.
  • Removes oxidation and corrosion to produce a bright, chemically clean surface.
  • Suitable for brush, immersion, and spray application.
  • Prepares aluminum for welding, painting, and chemical conversion coatings.
  • Compatible with BONDERITE® M-CR 1201 and BONDERITE® M-CR 1001 conversion coatings.

Applications / Suitable for

  • Aluminum cleaning
  • Aluminum brightening
  • Prepaint conditioning
  • Surface preparation before welding
  • Surface preparation before painting
  • Pretreatment before chemical conversion coating

Technical Specifications

General Properties
Product Type
Material category or functional product class.
Phosphoric acid cleaner & brightener
Thermal Properties
Operating Temperature
Ambient to 140°F (60°C) °C

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Method / Condition
Technology Acid deoxidizer — Supplier classification
Product type Phosphoric acid-based cleaner, brightener and prepaint conditioner — Supplier description
Application Aluminum cleaning and conditioning — Supplier classification
Brush dilution (light oxidation) 1:5 Product : Water Brush application
Brush dilution (heavy oxidation) 1:2 Product : Water Brush application
Immersion bath preparation 25:75 Product : Water Per 100 parts bath
Spray dilution 1:3 Product : Water 62-G applicator setting 3
Storage Protect from freezing below -9°C (15°F); thaw and stir before use if frozen — Supplier recommendation
Shelf life Not stated — Technical Process Bulletin
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Method / Condition
Surface condition Chemically clean, bright, corrosion-free aluminum surface — After treatment
Typical contact time 2–5 minutes Typical treatment
Application temperature Ambient to 49 °C Room temperature to 120°F
Application methods Brush, immersion, spray — Supplier recommendation
Recommended follow-on processes Welding, painting, BONDERITE® M-CR 1201 or BONDERITE® M-CR 1001 conversion coating — After rinsing