BONDERITE C-IC 2310

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

BONDERITE C-IC 2310

Main features

  • Chromium-Free Aluminum Deoxidizing Cleaner
  • No-Heat Immersion/Spray Cleaning
  • MIL-W-6858C Deoxidizing Compliance

Product Description

BONDERITE® C-IC 2310 is a chromium-free concentrated acidic cleaner formulated for deoxidizing and desmutting wrought aluminum alloys. It effectively removes surface oxides, heat-treatment discoloration, thermal deburring residue, and smut generated during alkaline etching and chemical milling. The process produces a stain-free aluminum surface prior to anodizing, chemical milling, penetrant inspection, and resistance welding, while operating efficiently without heating and performing well in both immersion and spray systems. :contentReference[oaicite:0]{index=0}

Key Features

  • Chromium-free acidic formulation for deoxidizing and desmutting wrought aluminum alloys.
  • Removes oxides, heat-treatment discoloration, and alkaline etch smut while producing a stain-free surface.
  • Requires no heating and rinses freely after treatment.
  • Suitable for immersion and agitated spray systems due to its non-foaming formulation.
  • Meets MIL-W-6858C Paragraph 4.2 deoxidizing requirements and numerous aerospace specifications.

Applications / Suitable for

  • Wrought aluminum alloys
  • Deoxidizing after alkaline etching
  • Desmutting after chemical milling
  • Anodizing pretreatment
  • Chemical milling pretreatment
  • Penetrant dye inspection pretreatment
  • Spot and resistance welding pretreatment

Technical Specifications

General Properties
Product Type
Material category or functional product class.
Chromium-free acidic deoxidizer
Thermal Properties
Operating Temperature
Ambient (room temperature) °C

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Method / Condition
Technology Acid cleaner — Supplier classification
Product type Chromium-free concentrated acidic liquid — Supplier description
Application Deoxidizing and desmutting — Supplier classification
Bath make-up 15 gal per 100 gal Initial bath preparation
Nitric acid addition 25 gal per 100 gal 42° Bé nitric acid
Storage Protect from freezing below -1°C (30°F); thaw completely and stir before use if frozen — Supplier recommendation
Shelf life Not stated — Technical Process Bulletin
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Method / Condition
Surface finish Stain-free deoxidized and desmutted aluminum surface — After treatment
BONDERITE C-IC 2310 concentration 10–20 % by volume Working bath
Nitric acid concentration 20–30 % by volume 42° Bé nitric acid
Operating temperature 15–32 °C 60–90°F
Treatment time 2–10 minutes Immersion
Etch rate 0.1–0.4 mils/surface/hour 2024 clad aluminum panel
Application method Immersion with air or mechanical agitation — Filtration recommended