BONDERITE C-AK 909

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

BONDERITE C-AK 909

Main features

  • Heavy-Soil Multi-Metal Degreasing
  • Immersion or Ultrasonic Cleaning
  • Caustic-Soda-Free Chelating Formulation

Product Description

BONDERITE® C-AK 909 is a moderately alkaline powdered cleaner formulated for degreasing heavily soiled metal surfaces without attacking the underlying substrate. Suitable for steel, copper, zinc, aluminum, stainless steel, titanium, and other metals, it is used during surface preparation before chemical conversion coatings, electroplating, welding, metal brightening, and other finishing operations. The cleaner offers strong chelating and surface-tension-reducing properties while remaining free of caustic soda, and can be applied by immersion or ultrasonic cleaning.

Key Features

  • Multi-metal compatibility: Suitable for steel, copper, zinc, aluminum, stainless steel, titanium, and other metals.
  • Moderately alkaline formulation: Degreases heavily soiled metal surfaces without attacking the substrate.
  • Strong cleaning chemistry: Combines chelating and surface-tension-reducing properties for effective contaminant removal.
  • Caustic soda free: Formulated with alkaline salts without caustic soda.
  • Flexible processing: Suitable for both immersion and ultrasonic cleaning systems.

Applications / Suitable for

  • Surface preparation before chemical conversion coating
  • Cleaning before chemical or electrolytic deposition
  • Cleaning before welding
  • Metal brightening operations
  • Immersion degreasing
  • Ultrasonic degreasing

Technical Specifications

Other Properties
Storage Temperature
0–40°C °C
General Properties
Appearance
Appearance at room temperature.
Amber liquid
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
Not Published

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Typical supplier-published characteristics of BONDERITE® C-AK 909.

Property Value Unit Method / Condition
Technology Industrial Cleaner — Supplier classification
Product Type Alkaline Cleaner — Supplier classification
Application Metal Cleaner — Supplier classification
Appearance Powder — As supplied
Color White / Cream — Typical property
Water Solubility Easy — Typical property
pH (10 g/L solution) ~12.5 — Typical property
Chemistry Alkaline salts without caustic soda — Supplier description
Storage Temperature 0–40 °C Recommended storage
Shelf Life 24 months Unopened original packaging
Technical Properties

After-Processing / Operating Properties

Typical supplier-recommended operating parameters for BONDERITE® C-AK 909.

Property Value Unit Method / Condition
Immersion concentration 40–80 g/L Degreasing by immersion
Immersion temperature 50–90 °C Recommended operating range
Immersion contact time 5–15 minutes Recommended operating range
Ultrasonic concentration 20–40 g/L Degreasing by ultrasound
Ultrasonic temperature 50–80 °C Recommended operating range
Ultrasonic contact time 2–5 minutes Recommended operating range
Bath control Concentration (g/L) = 7.2 × mL of 1 N HCl — Methyl orange titration
Total alkalinity (50 g/L bath) Approx. 7 points Typical bath value
Replenishment 720 g per point Add product to increase bath alkalinity by 1 point