BONDERITE C-AK 5948-DPM

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

BONDERITE C-AK 5948-DPM

Main features

  • Painted/Unpainted Aircraft Cleaning
  • Nonstaining Free-Rinsing Aluminum Cleaning
  • Phosphate/Chromate-Free Immersion/Ultrasonic Cleaning

Product Description

BONDERITE® C-AK 5948DPM EU AERO is a blue, water-based alkaline cleaner concentrate formulated for cleaning painted and unpainted aircraft exterior and interior surfaces after dilution with water. Designed for immersion and dip applications, it is suitable for aircraft metals and well-bonded paint and can be used in ultrasonic parts-cleaning tanks. The free-rinsing formulation is readily soluble and stable in water mixtures, provides nonstaining and nonstreaking cleaning on aluminum, and does not contain phosphates, chromates, or butyl cellosolve.

Key features

  • Aircraft-surface cleaning: Formulated for painted and unpainted aircraft exterior and interior surfaces.
  • Broad aircraft-material suitability: Suitable for aircraft metals and well-bonded paint.
  • Aluminum appearance protection: Provides nonstaining and nonstreaking cleaning on aluminum under suitable process conditions.
  • Free-rinsing water-based formulation: Readily soluble and stable in water mixtures for efficient rinsing after cleaning.
  • Restricted-substance formulation: Does not contain phosphates, chromates, or butyl cellosolve.

Applications / Suitable for

  • Painted and unpainted aircraft exterior surfaces
  • Aircraft interior surfaces
  • Aircraft metals and well-bonded paint
  • Immersion and dip cleaning
  • Ultrasonic parts-cleaning tanks
  • Metal pretreatment processes

Technical Specifications

Other Properties
Storage Temperature
0–35°C °C
General Properties
Appearance
Appearance at room temperature.
Blue liquid
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.006–1.026 g/mL

Additional Information

Technical properties

As-supplied / before-processing properties

Supplier-published characteristics and storage information for BONDERITE® C-AK 5948DPM EU AERO.

Property Value Unit Method / condition
Technology Metal pretreatment — Supplier classification
Product type Alkaline cleaner — Supplier classification
Application Immersion — Supplier classification
Appearance Blue liquid — As supplied
pH 11.4–12.2 — Supplier-published technical data
Density 1.006–1.026 g/mL Supplier-published technical data
Flammability Nonflammable — Supplier-listed feature
Restricted constituents No phosphates, chromates, or butyl cellosolve — Supplier-listed formulation feature
Storage temperature 0–35 °C Store cool, frost-free, and in the original sealed container
Frost sensitivity Frost-sensitive — Storage requirement
Technical properties

After-processing / operating properties

Supplier-published operating and bath-control conditions for immersion cleaning with BONDERITE® C-AK 5948DPM EU AERO.

Property Value Unit Method / condition
Dilution ratio 1 part cleaner to 3–20 parts water — Selected according to soil load
Operating temperature 65–80 °C Immersion cleaning
Contact time 5–15 minutes Immersion cleaning
Ultrasonic compatibility Suitable — Supplier identifies product as ideal for ultrasonic tanks
Bath-control sample volume 100 mL Titrate bath sample with 1.0 N sulfuric acid
Bath-control endpoint 8 pH Endpoint using 1.0 N H₂SO₄
Bath concentration calculation V × 2.06 % V = volume of 1.0 N sulfuric acid used in the titration