BONDERITE C-AK 4338LP1

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

BONDERITE C-AK 4338LP1

Main features

  • Two-Part Alkaline-Permanganate System Component
  • Jet-Engine Heat-Scale Conditioning
  • Liquid-Concentrate Bath Make-Up

Product Description

BONDERITE® C-AK 4338L AERO (Part 1) is the Part 1 component of a two-component alkaline permanganate scale remover and conditioner developed specifically for jet engine cleaning. Used together with BONDERITE® C-AK 4338L AERO Part 2, it chemically modifies high-temperature oxide scale on ferrous and heat-resistant alloys to condition deposits for efficient removal during subsequent chemical processing. The liquid concentrate is supplied for safer handling than powdered products and is suitable for both bath make-up and bath maintenance.

Key Features

  • Part of a two-component conditioning system for high-temperature oxide scale removal.
  • Developed for jet engine cleaning and metal pretreatment operations.
  • Suitable for ferrous and heat-resistant alloys under controlled process conditions.
  • Liquid concentrate for safer handling and easier bath preparation than powdered alternatives.
  • Long bath life with supplier-stated REACH compliance.

Applications / Suitable for

  • Jet engine cleaning
  • High-temperature oxide scale conditioning
  • Ferrous alloys
  • Heat-resistant alloys
  • Metal pretreatment processes
  • Immersion processing as part of the BONDERITE® C-AK 4338L AERO system

Technical Specifications

Other Properties
Storage Temperature
Optimum 19–24°C (protect from freezing) °C
General Properties
Appearance
Appearance at room temperature.
Colorless liquid
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
Not Published

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Method / Condition
Technology Metal pretreatment — Supplier classification
Chemical type Permanganate scale remover / conditioner — Supplier classification
Component Part 1 of two-component system — Used with Part 2 in equal volumes
Appearance Colorless — Part 1 as supplied
Application Metal pretreatment — Supplier classification
Specific benefit Long bath life — Supplier feature
Alloy compatibility Ferrous and heat-resistant alloys — Do not use on reactive alloys such as aluminum
Optimal storage 19–24 °C Protect from freezing
Technical Properties

After-Processing / Operating Properties

Property Value Unit Method / Condition
Part 1 working concentration 15–25 % by volume Final working solution
Mix ratio Equal volume with Part 2 — Part 1 added to water before Part 2
Solution preparation temperature 90 °C Heat while mixing
Operating temperature 80–95 °C Immersion scale-conditioning step
Immersion time 30–60 minutes Published process sequence
Bath concentration calculation [(2 × A) − B] × 1.05 % by volume Part 1 titration using 1.0 N sulfuric acid
Compatible tank material Mild steel — Supplier recommendation

Leading Brands Trust in Our Products and Services