BONDERITE C-AK 4316

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

BONDERITE C-AK 4316

Main features

  • Heat-Scale Conditioning for Multiple Alloys
  • Lower-Temperature Molten-Salt Bath Processing
  • Nonflammable Titration-Controlled Bath Maintenance

Product Description

BONDERITE® C-AK 4316 AERO is a light yellow granular alkaline cleaner developed to condition heat scale and thermal oxides on ferrous metals, stainless steels, magnesium alloys, and titanium alloys prior to pickling. The immersion process provides scale conditioning comparable to conventional molten salt baths while operating at lower temperatures and lower cost per part. The readily soluble formulation is nonflammable, rinses easily with cold water, and is controlled by titration for consistent bath maintenance.

Key Features

  • Conditions heat scale and thermal oxides prior to pickling of selected engineering alloys.
  • Lower-temperature alternative to conventional molten salt baths.
  • Readily soluble granular formulation with titration-based bath control.
  • Cold-water rinsing following immersion processing.
  • Nonflammable in both granular form and working solution.

Applications / Suitable for

  • Conditioning heat scale prior to pickling
  • Ferrous metals
  • Stainless steels
  • Magnesium alloys
  • Titanium alloys
  • Immersion metal pretreatment processes

Technical Specifications

Other Properties
Storage Temperature
0–40°C °C
General Properties
Appearance
Appearance at room temperature.
Light yellow granular compound
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
Not Published

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Method / Condition
Technology Metal Pretreatment — Supplier classification
Product Type Alkaline Cleaner — Supplier classification
Application Immersion process — Supplier classification
Appearance Light yellow granular compound — As supplied
Physical form Readily soluble powder — Supplier description
Flammability Nonflammable — Granular form and solution
Storage temperature 0–40 °C Recommended storage
Shelf life 24 months Original unopened packaging
Technical Properties

After-Processing / Operating Properties

Property Value Unit Method / Condition
Working concentration 760–775 g/L Immersion bath preparation
Operating temperature 140–145 °C Optimum operating range
Processing time (oxides formed below 650°C) 10–15 minutes Immersion processing
Processing time (oxides formed above 650°C) 40–50 minutes Immersion processing
Rinse Cold overflowing water 3–5 minutes After treatment
Tank material Stainless steel — Mechanical agitation recommended
Bath control Titration with 1.0 N sulfuric acid — Concentration maintained by titration
Bath concentration calculation mL acid to pH 11 × 22.38 g/L Supplier calculation
Bath maintenance Maintain concentration by adding fresh material — Supplier recommendation

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers