BONDERITE C-AK 4181-L

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

BONDERITE C-AK 4181-L

Main features

  • Single-Step Rust and Corrosion Removal
  • Immersion, Electrolytic, or Ultrasonic Use
  • AMS-1379 Aerospace Specification Testing

Product Description

BONDERITE C-AK 4181 L AERO is a liquid, strongly alkaline immersion cleaner that rapidly removes rust, corrosion, heat discoloration, grease, and dirt deposits from metal surfaces in a single step. It serves as a liquid alternative to the powder-based BONDERITE C-AK 4181 AERO, simplifying storage and handling. The cleaner is suited for cast steel, steel, iron, stainless steel, titanium, cadmium, magnesium, and copper alloys, and can be used in immersion, electrolytic, or ultrasonic processes. Steel components do not discolor and hydrogen embrittlement does not occur on iron or steel. The product has been tested to AMS-1379 and multiple aerospace OEM specifications, and it has a pH above 13 with a density of 1.3 g/mL.

Key features

  • Single-Step Rust and Corrosion Removal: rapidly and economically removes rust, corrosion, heat deposits, grease, and dirt in one step
  • Immersion, Electrolytic, or Ultrasonic Use: can be used in normal immersion, electrolytic, or ultrasonic processes
  • Aerospace Specification Testing: tested to AMS-1379 and multiple aerospace OEM process specifications, including CFM, GE, and Pratt and Whitney SPMC requirements

Applications

Applications include industrial metal cleaning and alkaline rust removal on cast steel, steel, iron, stainless steel, titanium, cadmium, magnesium, and copper alloys, prior to further processing in immersion, electrolytic, or ultrasonic operations.

Product Family

BONDERITE C-AK 4181-L

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Slightly turbid liquid with light sediment at room temperature
Density (g)
1.3 g/cm3
Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
Not Applicable °C

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
Physical stateLiquidAs supplied
AppearanceClear, colorlessAs supplied
pH9.0 to 9.5As supplied
Specific gravity1.05 to 1.0920 deg C, as supplied
Flash pointAbove 190 (above 374)deg C (deg F)As supplied
VOC content5.4%Calculated, as supplied