BONDERITE C-AD-ETCH

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

BONDERITE C-AD-ETCH

Main features

  • Smooth Aluminum Etching for Anodizing
  • Adjustable Etch-Factor Additive Concentration
  • Concentrated Sodium-Hydroxide Etchant Additive

Product Description

BONDERITE® C-AD ETCH ADD3 AERO is a concentrated liquid additive and surfactant developed for use with sodium hydroxide to prepare aluminum-alloy etchant solutions. When used as directed in BONDERITE® etchant formulations, it produces smoothly etched aluminum surfaces suitable for subsequent finishing operations such as anodizing and chemical conversion coating. The concentrated formulation allows the etch factor to be adjusted for different process requirements while providing excellent line definition on selected aluminum alloys.

Key Features

  • Aluminum etchant additive designed for use with sodium hydroxide-based BONDERITE® etchant formulations.
  • Supports downstream finishing by producing smoothly etched aluminum surfaces suitable for anodizing and conversion coating.
  • Adjustable etch characteristics through concentration changes within approved BONDERITE® etchant formulations.
  • Highly concentrated liquid that can be incorporated into multiple BONDERITE® aluminum etchant formulations.
  • Cold-weather crystallization is reversible by warming the product or adding it directly to the operating etch tank.

Applications / Suitable for

  • Preparation of aluminum alloy etchant solutions
  • Chemical etching of aluminum alloys
  • Surface preparation before anodizing
  • Surface preparation before chemical conversion coating
  • BONDERITE® ETCHANT 9H, 11-L, and 17-L formulations
Product Family

BONDERITE C-AD-ETCH

Loading pricing…

Technical Specifications

Other Properties
Storage Temperature
Store below 50°C °C
General Properties
Appearance
Appearance at room temperature.
Reddish dark brown liquid
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.395 ± 0.01

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Supplier-published characteristics of BONDERITE® C-AD ETCH ADD3 AERO.

Property Value Unit Method / Condition
Product type Additive / Surfactant — Supplier classification
Appearance Reddish, dark brown liquid — As supplied
Specific gravity 1.395 ± 0.01 — Typical property
Solids content 49.5 % by weight Typical property
Weight per gallon 11.6 ± 0.1 lb/gal Typical property
Concentrate condition Highly concentrated liquid — May crystallize during cold weather without affecting activity
Storage Store below 50 °C Keep closed and away from acids, strong oxidizers, aluminum, tin, and zinc
Technical Properties

After-Processing / Operating Properties

Supplier-published formulation and operating information for BONDERITE® C-AD ETCH ADD3 AERO.

Property Value Unit Method / Condition
Primary use Used with sodium hydroxide etchant solutions — For aluminum alloy etching
BONDERITE ETCHANT 9H formulation 1.0 L per 100 L bath Published formulation
BONDERITE ETCHANT 11-L formulation 17.9 L per 100 L bath Published formulation
BONDERITE ETCHANT 17-L formulation 5.0 L per 100 L bath Published formulation
Bath maintenance Maintain N-1 and N-2 within formulation limits — Supplier process control
Etch-factor adjustment Varied by changing additive concentration — Within approved BONDERITE® formulations
Typical etch factor (2024-T3 clad) 0.87 (with grain), 0.75 (across grain) — TURCOFORM ETCHANT 11-L formulation
Typical etch factor (6061-T6) 0.92 (with grain), 0.89 (across grain) — TURCOFORM ETCHANT 11-L formulation
Observed surface quality Excellent line definition with no apparent end-grain pitting — Supplier evaluation