BIOACT EC-88

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

BIOACT EC-88

Main features

  • Broad Inline Defluxing
  • Non-Foaming High-Loading Wash Bath
  • 10 to 25% Aqueous Concentration

Product Description

BIOACT EC-88 is a proprietary, inherently non-foaming aqueous defluxer developed for high-throughput inline spray-in-air cleaning equipment. Used at 10–25% concentration in water, it removes lead-free, no-clean, RMA, water-soluble, and HMP flux residues, along with fingerprint oils, white residues, and ionic contamination. BIOACT EC-88 combines high flux-loading capacity with long wash-bath life and does not require defoamer or pH-booster additives. Typical process temperatures are 50–70°C for both the wash bath and DI-water rinse, supporting controlled post-solder cleaning of PCB assemblies in aqueous inline systems.

Key features

  • Inline spray-in-air defluxing: Specifically designed for aqueous inline spray-in-air cleaning equipment.
  • Broad flux-residue removal: Removes lead-free, no-clean, RMA, water-soluble, and HMP flux residues.
  • Ionic and process-soil removal: Removes ionic contamination, fingerprint oils, and white residues.
  • Inherently non-foaming: Supports inline spray processing without a separate defoamer.
  • High flux-loading capacity: Supports long wash-bath life under a controlled cleaning process.
  • No bath additives required: Does not require defoamer or pH-booster additives to maintain the documented process.

Applications / Suitable for

  • Aqueous inline spray-in-air defluxing
  • Post-solder cleaning of PCB assemblies
  • Removal of lead-free, no-clean, RMA, water-soluble, and HMP flux residues
  • Removal of white residues, fingerprint oils, and ionic contamination
Product Family

BIOACT EC-88

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
None to Boiling °C
General Properties
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
0.955
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
12 mPa.s

Additional Information

Surface Treatments | Aqueous Inline Defluxer

BIOACT EC-88

BIOACT EC-88 is an inherently non-foaming aqueous defluxer for high-throughput inline spray-in-air equipment. The concentrated cleaner removes multiple flux-residue types and ionic contamination while supporting high flux loading, long wash-bath life, and operation without defoamer or pH-booster additives.

Inline spray-in-air 10–25% concentration pH 10.3 at 15% 12 cP at 25°C Non-foaming

Vanatge Can

Product data

As-Supplied Properties

Typical product data for evaluation. These values are not guaranteed specifications.

Property Value Unit Method / condition
Odor Mild — As supplied
Flash point None to boiling — Typical product data
Specific gravity 0.955 — 25°C
pH 10.3 — 15% concentration
Viscosity 12 cP 25°C
Chemical oxygen demand 213 ppm 0.01% concentration
Application

Inline Cleaning Process

Use BIOACT EC-88 in aqueous inline spray-in-air equipment. Establish concentration, wash temperature, DI-water rinse temperature, conveyor settings, spray pressure, and bath-management controls for the assembly, flux chemistry, soil loading, and required cleanliness endpoint.

Wash-bath concentration: Dilute BIOACT EC-88 to 10–25% concentration in water.
Wash-bath temperature: Operate at 50–70°C (120–160°F).
DI-water rinse temperature: Operate at 50–70°C (120–160°F).
 

Inline Defluxing Sequence

Stage 1
Prepare the wash bath
Prepare a 10–25% BIOACT EC-88 solution in water and heat the wash section to 50–70°C (120–160°F). Confirm concentration and equipment compatibility.
Stage 2
Run the inline spray process
Process PCB assemblies through the aqueous inline spray-in-air system using validated conveyor speed, spray pressure, nozzle configuration, and exposure time.
Stage 3
Rinse and verify cleanliness
Rinse with DI water at 50–70°C (120–160°F), then verify the required ionic, visual, and process-cleanliness endpoint before downstream handling.
Storage and Handling

Store BIOACT EC-88 in its original, sealed container above 50°F (10°C) and protect the product from freezing. The documented shelf life is 36 months under these conditions. Standard packages include 40 lb (18 kg) pails and 440 lb (200 kg) drums. Consult the current SDS for complete handling, storage, exposure-control, spill-response, and disposal requirements.

Environmental and Regulatory Profile

Issue or observation Source-supported guidance Qualification boundary
Ozone depletion potential Zero Supplier-reported product environmental profile.
Global warming potential Low Supplier-reported qualitative classification.
Volatile organic compound 780 g/L Confirm current regional and process-specific VOC requirements.
Hazardous air pollutant No Supplier-reported product status.
SARA Not regulated Confirm current jurisdictional, facility, and process applicability.
Nonylphenol ethoxylates None Supplier-reported formulation attribute.
Alkylphenol ethoxylates None Supplier-reported formulation attribute.

Defluxing and Bath Guidance

Supported flux and process soils
BIOACT EC-55removes lead-free, no-clean, RMA, water-soluble, and HMP flux residues, plus fingerprint oils, white residues, and ionic contamination. Confirm the actual flux chemistry, assembly materials, residue condition, and cleanliness requirement.
Bath loading and additive control
The formulation is inherently non-foaming and is documented for high flux-loading capacity and long wash-bath life without defoamer or pH-booster additives. Establish site-specific concentration, contamination, filtration, and bath-change controls.
Supported use contexts

Applications

BIOACT EC-88 supports aqueous inline spray-in-air cleaning where flux residues, white residues, fingerprint oils, or ionic contamination must be removed from compatible PCB assemblies under a controlled production process.

Inline PCB defluxing
Use in aqueous inline spray-in-air equipment for high-throughput removal of supported lead-free, no-clean, RMA, water-soluble, and HMP flux residues.
Post-solder cleaning
Clean PCB assemblies after applicable soldering operations using a validated 10–25% wash solution and 50–70°C wash and DI-water rinse stages.
Residue and ionic-contamination removal
Remove documented white residues, fingerprint oils, and ionic contamination and verify the required visual and ionic-cleanliness endpoint.
Next steps

Technical Support

Work with Krayden to evaluate BIOACT EC-88 against your flux chemistry, PCB materials, inline cleaning equipment, throughput, wash concentration, temperature, rinse configuration, bath loading, and cleanliness targets. Our team can help review process trials, packaging, sampling, and implementation requirements.

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers