BIOACT CCR-8

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

BIOACT CCR-8

Main features

  • No-Heat Coating Removal
  • Manual or Immersion Cleaning
  • Controlled Solvent Evaporation

Product Description

BIOACT CCR-8 Conformal Coating Remover is a ready-to-use, bio-based solvent liquid for removing selected acrylic and silicone conformal coatings from printed circuit boards and electronic components. It works at full concentration without heating and can be applied by brush, pad, or cloth, or used in immersion equipment with controlled ultrasonic agitation. The 0.86 specific-gravity liquid combines a 120 deg F flash point with a controlled 304 to 372 deg F boiling range, supporting manageable evaporation during cleaning. It also removes supported flux residues, silicones, SMT adhesives, mold-release compounds, and uncured solder paste. Process suitability remains specific to the coating, substrate, component, and cleaning method.

Key Features

  • No-heat coating removal: Manual and immersion processes operate at full concentration without required heating.
  • Manual or immersion cleaning: Application options include brush, pad, cloth, immersion, and controlled ultrasonic agitation.
  • Multiple residue types: Targets selected coatings, flux residues, silicones, SMT adhesives, and uncured solder paste.

Applications

Removal of selected acrylic and silicone conformal coatings and supported electronics-process residues from PCBs and components.

Product Family

BIOACT CCR-8

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

Thermal Properties
Boiling Point
The amount of degree’s needed to reach in order to make the substance boil.
151-189 °C
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
49 °C
General Properties
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
0.86

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied liquid-cleaner properties and storage conditions.

PropertyValueUnitMethod / condition
OdorMild citrus-Typical
Flash point120 (49)deg F (deg C)Typical
Boiling point304 to 372 (151 to 189)deg F (deg C)760 mmHg
Specific gravity0.86-25 deg C
Volatile organic compound860g/LAs supplied
Shelf life36monthsOriginal sealed container above 50 deg F (10 deg C)

Leading Brands Trust in Our Products and Services