BIOACT 280E

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

BIOACT 280E

Main features

  • High-Melting Wax Removal
  • Multi-Polymer Cleaning Compatibility
  • Low-Odor Low-Volatility Cleaning

Product Description

BIOACT® 280E Precision Cleaner is a USDA Certified Biobased semi-aqueous cleaner formulated from a blend of aliphatic esters and surface-active agents. It is designed to dissolve paraffinic, microcrystalline, plating, and thermoplastic fixturing waxes while also removing pitches, greases, buffing compounds, metalworking fluids, coolants, hydraulic fluids, and lubricating oils. The low-odor cleaner is suitable for heated immersion cleaning and is compatible with many polymeric substrates, elastomers, and ferrous and non-ferrous alloys.

Key features

  • High-melting soil removal: Dissolves paraffinic, microcrystalline, plating, and thermoplastic fixturing waxes.
  • Broad material compatibility: Suitable for many polymeric substrates, elastomers, and ferrous and non-ferrous alloys.
  • High wax-loading capacity: Supports wax loading levels of up to 40%.
  • Low-volatility formulation: Provides very low odor, a vapor pressure below 0.002 mmHg at 20°C, and a flash point of 285°F (141°C).

Applications / Suitable for

  • Removal of paraffinic, microcrystalline, plating, and fixturing waxes
  • Removal of pitches, greases, coolants, hydraulic fluids, polishing compounds, buffing compounds, metalworking fluids, and lubricating oils
  • Heated immersion cleaning processes
  • Replacement of selected vapor-degreasing solvents and hot-oil dewaxing processes
Product Family

BIOACT 280E

Loading pricing…

Technical Specifications

Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
141 °C
General Properties
Vapor Pressure
<0.002 mmHg
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
7.3 mPa.s

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied and process properties. Values are not intended for use as specifications.

Property Value Unit Method / condition
Product type Semi-aqueous precision cleaner based on aliphatic esters and surface-active agents — As supplied
Odor Very low — Typical value
Flash point 285 (141) °F (°C) Typical value
Specific gravity 0.86 — At 25°C
Vapor pressure <0.002 mmHg At 20°C
Viscosity 7.3 cPs At 25°C
Kauri-butanol value 90 — Typical value
Volatile organic compound content 70 g/L Reported in the supplied TDS
Recommended wash-bath concentration 100 % Heated immersion cleaning
Recommended wash-bath temperature 190–205 (88–96) °F (°C) Heated immersion cleaning
Recommended DI-water rinse temperature 190–205 (88–96) °F (°C) Following heated immersion cleaning
Shelf life 36 months Original sealed container stored above 50°F (10°C); protect from freezing

Leading Brands Trust in Our Products and Services