BIOACT 280

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

BIOACT 280

Main features

  • High-Melting Wax Removal
  • 88 to 96 deg C Immersion Cleaning
  • Aerospace Process Acceptance

Product Description

BIOACT 280 Wax Remover is a semi-aqueous cleaner based on aliphatic esters and surface-active agents for heated immersion dewaxing. It quickly dissolves paraffinic and microcrystalline plating waxes and thermoplastic fixturing waxes, while also removing pitches, greases, buffing compounds, metalworking fluids, hydraulic fluids, coolants, and lubricating oils. The product is used at full concentration in heated immersion equipment, with mechanical agitation and heated DI-water rinsing. Typical data include a 141°C flash point, very low odor, vapor pressure below 0.002 mmHg at 20°C, and wax loading up to 40%. It is compatible with many polymers, elastomers, and ferrous and non-ferrous alloys and is documented for multiple aerospace processes.

Key features

  • Heated immersion wax removal: Designed for full-strength use in heated immersion and soak-tank equipment.
  • High-melting wax solvency: Dissolves paraffinic and microcrystalline plating waxes and thermoplastic fixturing waxes.
  • Wax loading capability: Documented for wax loading up to 40%.
  • High flash point and very low vapor pressure: Typical flash point of 141°C and vapor pressure below 0.002 mmHg at 20°C.
  • Broad material compatibility: Documented for many polymers and elastomers and for ferrous and non-ferrous alloys.
  • Aerospace process acceptance: Documented for GE Aviation, Honeywell, IAE, Pratt & Whitney, and related aerospace testing requirements.

Applications / Suitable for

  • Removal of paraffinic and microcrystalline plating waxes
  • Removal of thermoplastic fixturing waxes
  • Heated immersion cleaning of aerospace and precision components
  • Removal of pitches, greases, buffing compounds, metalworking fluids, hydraulic fluids, coolants, and lubricating oils
Product Family

BIOACT 280

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
163.5 °C
General Properties
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
0.87
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
7.3 mPa.s

Additional Information

Surface Treatments | Semi-Aqueous Wax Remover

BIOACT 280 Wax Remover

BIOACT 280 Wax Remover is a semi-aqueous cleaner for heated immersion removal of paraffinic and microcrystalline plating waxes and thermoplastic fixturing waxes. Its high flash point, very low vapor pressure, documented wax loading, and material compatibility support aerospace and precision dewaxing processes.

Semi-aqueous cleaner 141°C flash point <0.002 mmHg vapor pressure 7.3 cP at 25°C Up to 40% wax loading

Vantage Can

Product data

As-Supplied Properties

Typical product data for evaluation. These values are not guaranteed specifications.

Property Value Unit Method / condition
Odor Very low — As supplied
Flash point 141 (285) °C (°F) Typical product data
Specific gravity 0.87 — 25°C
Vapor pressure <0.002 mmHg 20°C
Viscosity 7.3 cP 25°C
Kauri-Butanol value 90 — Typical solvency value
Application

Application and Processing

Use BIOACT 280 at full concentration in heated immersion equipment. Control bath temperature, agitation, rinsing, and material compatibility according to the wax, component geometry, substrate, and applicable aerospace process.

Wash-bath concentration: 100% concentration.
Wash-bath temperature: 88–96°C (190–205°F) for wax removal.
DI-water rinse temperature: 88–96°C (190–205°F). Mechanical agitation is recommended.

 

Wax-Removal Sequence

Stage 1
Prepare the heated wash bath
Charge the immersion tank with BIOACT 280 at full concentration and heat the bath to 88–96°C (190–205°F) for wax-removal operations.
Stage 2
Dissolve the wax
Immerse the component and use air, liquid, or mechanical agitation as appropriate. Lower temperatures may be evaluated for oil and grease removal.
Stage 3
Complete the heated rinse
Remove the cleaner with a heated DI-water rinse at 88–96°C (190–205°F). Many systems use two or three successive rinses; verify cleanliness before the next process.
Storage and Handling

Store BIOACT 280 in its original, sealed container at or above 50°F (10°C) and protect the product from freezing. The documented shelf life is 36 months under these conditions. Standard packages include 36 lb (16 kg) pails and 400 lb (181 kg) drums. Consult the current SDS for safe handling, exposure controls, storage, and disposal requirements.

Environmental Profile

Issue or observation Source-supported guidance Qualification boundary
Ozone depletion potential Zero Product environmental-profile value.
Global warming potential Essentially zero Supplier-reported product classification.
Hazardous air pollutant No Supplier-reported product status.
Volatile organic compound 137 g/L Verify applicable regional and process-specific VOC requirements.
SARA Not regulated Confirm current jurisdictional and facility obligations.
NESHAPs Not regulated Confirm current process and facility applicability.
RCRA Not regulated Waste classification depends on use and contamination; follow local requirements.

Technical Guidance

Documented soils
Documented cleaning targets include paraffinic wax, microcrystalline wax, plating wax, thermoplastic fixturing wax, pitches, greases, buffing and polishing compounds, metalworking fluids, hydraulic fluids, coolants, and lubricating oils.
Material and process compatibility
BIOACT 280 is documented for many polymeric substrates and elastomers and for ferrous and non-ferrous alloys. Confirm the exact alloy, polymer, elastomer, coating, bath temperature, exposure time, agitation, rinse sequence, and downstream process.

Approvals and Testing

Issue or observation Source-supported guidance Qualification boundary
General Electric Aviation General parts cleaner and plating wax remover on GEAE and CFMI engine hardware; Master Cleaner List 3.6.5, Semi-Aqueous Immersion Cleaners at 100% concentration. Use only within the identified hardware, process, list, and revision scope.
Honeywell Process Specification C7010, Rev H; conforms to EMS 53170 Rev C Type 1. Verify the current Honeywell process revision and exact application scope.
International Aero Engines IAE CoMat 01-460. Apply only within the named material and process requirements.
Pratt & Whitney MCL E-205 Titanium Stress Corrosion Test; PMC 8913-1,-2 for SPOP 37 Method 2 plating-wax removal and POP 1800-U masking-process use. Preserve the exact part, process, method, and revision boundaries.
Testing and additional support ASTM F1110, F2111, F945, and F519; supported by Hawker Pacific Aerospace, U.K. as a general-purpose high-temperature degreasing agent. Testing and support statements do not establish universal material or process suitability.
Supported use contexts

Applications

BIOACT 280 supports heated immersion cleaning where plating waxes, fixturing waxes, and related high-melting or oily soils must be removed from compatible aerospace and precision components.

Plating wax removal
Dissolves paraffinic and microcrystalline plating waxes used for selective processing of compatible components.
Fixturing wax removal
Removes thermoplastic fixturing waxes used to hold or support parts during machining and related manufacturing operations.
Heated immersion degreasing
Removes pitches, greases, buffing compounds, metalworking fluids, hydraulic fluids, coolants, polishing compounds, and lubricating oils from compatible parts.
Next steps

Technical Support

Work with Krayden to evaluate BIOACT 280 against your masking wax, substrate, immersion equipment, bath temperature, agitation, rinse sequence, and aerospace process requirements. Our team can help review compatibility, approvals, packaging, samples, and implementation conditions.

Leading Brands Trust in Our Products and Services