BERGQUIST TGF 3600

Harmonization Code : 3824.99.92.97 | Prepared binders for foundry molds or cores; chemical products and preparations of the chemical or allied industries (including those consisting of mixtures of natural products), not elsewhere specified or included: other : other : other

BERGQUIST TGF 3600

Main features

  • 3.6 W/m-K Thermal Conductivity
  • Sixty-Minute Application Window
  • Soft Conforming Gap Fill

Product Description

BERGQUIST GAP FILLER TGF 3600 is a two-component, 1:1 silicone liquid gap filler for transferring heat between electronic components and housings or heat sinks. Its thixotropic mixed consistency supports precision dispensing, then flows under assembly pressure to conform around irregular topography and fill interface gaps. Room-temperature or accelerated heat cure produces a soft, low-modulus elastomer with 3.6 W/m-K thermal conductivity and Shore 00 hardness of 35. A 60-minute pot life at 25 deg C supports controlled application, while the cured material maintains vertical gap stability across a -60 to 200 deg C operating range. It is intended for thermal coupling rather than structural attachment.

Key Features

  • 3.6 W/m-K heat transfer: Provides high bulk thermal conductivity after cure.
  • Conforming low-modulus interface: Flows under assembly pressure and cures to Shore 00 hardness of 35.
  • Ambient or accelerated cure: Cures at room temperature or on the specified heat schedule.

Applications

Thermal coupling of automotive electronics, PCB assemblies, discrete components, housings, and fiber-optic telecommunications equipment.

Technical Specifications

General Properties
Color
The color
Part A: White | Part B: Blue | Mixed: Blue
Component System
Describes the number of components that must be supplied, mixed, or activated before application or cure.
Silicone
Density (g)
3.0 g/cm3
Thermal Properties
Operating Temperature
(-)60 to 200 °C
Thermal Conductivity
Thermal conductivity describes the ability of a material to conduct heat. It is required by power packages in order to dissipate heat and maintain stable electrical performance. Thermal conductivity units are [W/(m K)] in the SI system and [Btu/(hr ft °F)] in the Imperial system.
(Cured) 3.6 W/m.K
Electrical Properties
Volume Resistivity
Volume resistivity, also called volume resistance, bulk resistance or bulk resistivity is a thickness dependent measurement of the resistivity of a material perpendicular to the plane of the surface.
(Cured) 1 x 10^8 Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

Uncured-system values; component and mixed colors are identified separately.

PropertyValueUnitMethod / condition
AppearancePart A: white; Part B: blue; mixed: blue-Visual
Mix ratio, Part A:Part B1:1 by weight; 1:1 by volumepartsTwo-component system
Mixed viscosity150,000mPa-s (cP)ASTM D2196; Brookfield RV Helipath; spindle TF; 20 rpm; 25 deg C
Density3.0g/ccASTM D792
Pot life60min25 deg C; time for viscosity to double
Shelf life5monthsUnopened containers at 25 deg C and 50% RH
Technical properties

After-processing / final-state properties

Cured-material values; thermal conductivity is a bulk material result under ASTM D5470.

PropertyValueUnitMethod / condition
Hardness35Shore 00ASTM D2240; 30-second delay
FlammabilityV-0UL 94Cured material
Dielectric strength275V/milASTM D149
Dielectric constant8.0-ASTM D150 at 1,000 Hz
Thermal conductivity3.6W/(m-K)ASTM D5470
Operating temperature range-60 to 200deg CCured material