AXAREL 2000

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

AXAREL 2000

Main features

  • MIL-PRF-680 Type II Approval
  • Hand-Wipe, Immersion, or Vacuum Cleaning
  • Low-Odor Low-Residue Soil Removal

Product Description

AXAREL 2000 Solvent Cleaner is a ready-to-use, low-odor hydrocarbon cleaner approved to MIL-PRF-680 Type II. It is designed for hand wiping, immersion cleaning, and compatible airless vacuum hydrocarbon equipment, where it removes greases, mineral oils, lubricants, coolants, synthetic soils, and particulate matter while leaving very low surface residues. AXAREL 2000 can be used for general cleaning and degreasing, maintenance operations, cleaning before non-destructive inspection, and surface preparation before bonding, painting, plating, sealing, welding, or additional processing. It is compatible with many polymeric substrates and elastomers and is suitable for ferrous and non-ferrous alloys.

Key features

  • MIL-PRF-680 Type II approved: Supports qualified aerospace, defense, and maintenance cleaning requirements.
  • Multiple cleaning methods: Suitable for hand wiping, immersion cleaning, and compatible airless vacuum hydrocarbon equipment.
  • Low-residue cleaning: Removes common oils, greases, coolants, synthetic soils, and particulate matter while leaving very low surface residues.
  • Low odor and low vapor pressure: Supports cleaning operations where reduced solvent odor and lower evaporative losses are important.
  • Broad material compatibility: Compatible with many polymeric substrates and elastomers and suitable for ferrous and non-ferrous alloys.

Applications / Suitable for

  • General-purpose parts cleaning and degreasing
  • Cleaning before non-destructive inspection, packaging, or final assembly
  • Surface preparation before bonding, painting, plating, sealing, welding, or further processing
Product Family

AXAREL 2000

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
62 °C
General Properties
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
0.77
Surface Tension
225.1 mN/m
Vapor Pressure
0.49 mmHg

Additional Information

Surface Treatments | Solvent Cleaner

AXAREL 2000 Solvent Cleaner

AXAREL 2000 is a ready-to-use, low-odor hydrocarbon cleaner approved to MIL-PRF-680 Type II. It supports manual, immersion, and compatible airless vacuum cleaning processes for removing oils, greases, coolants, synthetic soils, and particulate matter while leaving very low surface residues.

MIL-PRF-680 Type II Low odor 144 °F (62 °C) flash point Manual and immersion cleaning Very low surface residue

As-supplied properties

Typical physical properties

Typical values are provided for product evaluation and are not guaranteed specifications unless explicitly identified as such.

Property Value Unit Method / condition
Physical form Liquid — As supplied
Odor Essentially odorless — Typical
Flash point 144 / 62 °F / °C Closed cup
Specific gravity 0.77 — 25 °C
Viscosity 1.54 cP 25 °C
Kauri-butanol value 31 — Typical solvency index
Vapor pressure 0.49 mm Hg 20 °C
Non-volatile residue 30 ppm Typical
Processing

Cleaning methods and process use

Use AXAREL 2000 at full concentration. Select the cleaning method according to part geometry, soil loading, production requirements, and equipment compatibility. Verify material compatibility and the required cleanliness endpoint for the specific assembly before production use.

Manual cleaning: Apply at full concentration by brush, pad, or cloth, then allow the solvent to drain and evaporate according to the approved work instruction.
Immersion cleaning: Add at full concentration to the cleaning reservoir and use in a compatible immersion system. Manage soil loading and bath condition according to the equipment and process requirements.
Equipment use: Suitable for compatible airless vacuum hydrocarbon equipment. Confirm equipment compatibility, ventilation, ignition controls, and operating procedures before use.
Illustration of manual wiping, immersion cleaning, and airless vacuum cleaning methods for AXAREL 2000

Insert an approved processing visual showing manual, immersion, or compatible airless vacuum cleaning.

Storage and Handling

Keep the container tightly closed in a cool, well-ventilated area and away from heat, sparks, open flames, and other ignition sources. Follow the current safety data sheet, site solvent-handling procedures, applicable ventilation requirements, and all local regulations for storage, use, and disposal.

Cleaning performance

Low-residue cleaning across common maintenance soils

Soils removed
Oils, greases, coolants, synthetics, and particulates
Supports cleaning of common maintenance and manufacturing soils documented for the product.
Surface residue
30 ppm
Typical non-volatile residue value for processes requiring clean surfaces before inspection, assembly, or subsequent treatment.
Material compatibility
Metals, polymers, and elastomers
Documented as compatible with many polymeric substrates and elastomers and suitable for ferrous and non-ferrous alloys. Validate the exact material and finish before production use.
Approvals and conformance

Documented aerospace and defense references

Approval and specification status can change. Confirm the current revision, exact product designation, application, and required certification before use.

Organization / specification Documented reference
U.S. Military MIL-PRF-680 Type II Degreasing Solvent, Qualified Products List
Airbus A330 Maintenance Manual Item 11-002; Airbus Consumable Materials List reference to MIL-PRF-680
Boeing PSD 6-88 for BAC 5750
Lockheed Martin STP57-201 Rev H (EPS G41.14)
Pratt & Whitney PMC 9001-3, -4, -8
Rolls-Royce CSS276; OMat 102
Additional documented references Eurocopter; Goodrich Wheels and Brakes; Honeywell Aerospace; Messier-Bugatti
Next steps

Evaluate AXAREL 2000 for your cleaning process

Krayden can help review substrate compatibility, soil type, cleaning equipment, downstream process requirements, and applicable aerospace or defense specifications for AXAREL 2000.