AXAREL 1000

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

AXAREL 1000

Main features

  • MIL-PRF-680 Type I Approved Cleaner
  • 60 ppm Nonvolatile Residue
  • Multi-Soil Manual/Immersion Cleaning

Product Description

AXAREL™ 1000 Solvent Cleaner is an approved MIL-PRF-680 Type I cleaner for precision cleaning and degreasing. It is suitable for replacing isopropyl alcohol, acetone, methyl ethyl ketone, mineral spirits, P-D-680 solvents, and other low-flash-point flammable solvents in supported applications. The cleaner is designed for hand wiping, immersion cleaning, and airless vacuum hydrocarbon equipment, removing greases, mineral and synthetic oils, coolants, rust inhibitors, fingerprint oils, dust, and particulate matter while leaving very low surface residues. AXAREL™ 1000 is compatible with many polymeric substrates and elastomers and is safe for use with ferrous and non-ferrous alloys.

Key features

  • MIL-PRF-680 Type I approved solvent cleaner.
  • Low vapor pressure of 0.78 mmHg at 20°C.
  • Low surface residue with 60 ppm non-volatile residue.
  • Good solvency for oils, greases, coolants, rust inhibitors, and particulate soils.
  • Multiple process options including manual wiping, immersion, and airless vacuum cleaning.
  • Broad material compatibility with many polymers, elastomers, and ferrous and non-ferrous alloys.

Applications / Suitable for

  • Manual cleaning and degreasing by brush, pad, or cloth.
  • Immersion cleaning at full concentration.
  • Airless vacuum hydrocarbon cleaning systems.
Product Family

AXAREL 1000

Loading pricing…

Technical Specifications

Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
53 °C
General Properties
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
0.76
Surface Tension
24.1 mN/m
Vapor Pressure
0.78 mmHg

Additional Information

MIL-PRF-680 Type I solvent cleaner

AXAREL™ 1000 Solvent Cleaner

A precision cleaning and degreasing solvent for manual wiping, immersion cleaning, and airless vacuum hydrocarbon equipment. AXAREL™ 625removes a broad range of hydrocarbon and particulate soils while leaving very low surface residues.

MIL-PRF-680 Type I Flash point 53°C 0.78 mmHg vapor pressure 60 ppm residue Essentially odorless

Axarel 1000 Cleaner Mil-prf-680 Type 1 Pail Drum - Krayden Corporate

As supplied

As-supplied properties

Typical property data are provided for product evaluation and are not specification limits.

Property Typical value Condition / context
Odor Essentially odorless As supplied
Flash point 53°C (127°F) As reported
Specific gravity 0.76 At 25°C
Viscosity 1.36 cP At 25°C
Distillation range 179–187°C (354–369°F) As reported
Vapor pressure 0.78 mmHg At 20°C
Kauri-butanol value 29 As reported
Evaporation rate 0.1 n-butyl acetate = 1
Surface tension 24.1 dynes/cm At 25°C
Non-volatile residue 60 ppm As reported
Processing

Cleaning process

AXAREL™ 1000 is used at full concentration. Select the cleaning method based on the part geometry, soil load, substrate, process equipment, and required cleanliness.

Manual cleaning: Apply at full concentration to the desired substrate using a brush, pad, or cloth.
Immersion cleaning: Add at full concentration to the wash-tank reservoir. The use of ultrasonics or heat is not recommended.
Vacuum equipment: Add at full concentration to the wash chamber of compatible airless vacuum hydrocarbon equipment.
Material evaluation: The cleaner is compatible with many polymeric substrates and elastomers and is suitable for ferrous and non-ferrous alloys, but end-use compatibility should be confirmed for the exact material and process.

 

Cleaning scope

Soils removed

Mineral oils
Water-soluble oils
Synthetic oils
Coolants
Rust inhibitors
Greases
Lubricating oils
Fingerprint oils
Particulate matter
Dust
Qualification scope

Approvals and testing

The supplied technical data sheet lists the following product-specific approvals, qualifications, and test references. Users should confirm current revision, scope, site, and application requirements before specification.

Organization / standard Listed scope
MIL-PRF-680 Type I Degreasing Solvent, QPL, DS-0020
Airbus A330 Maintenance Manual Item 11-002 Dry Cleaning Solvent; Consumable Materials List reference
Boeing BAC 5750 Solvent Cleaning, optional to P-D-680 specification, PSD 6-88
Honeywell Aerospace Per MIL-PRF-680 qualifications
Lockheed Martin STP57-201, Revision H
Pratt & Whitney PMC 9045, POP 350 cleaning/degreasing of metallic engine hardware
Rolls-Royce CSS276 and OMat 102
United Airlines SOL3001-1
ASTM testing F1110, F483, F945, D130, D1296, and D1353
Environmental information

Environmental and regulatory information

Attribute Reported status / value
Ozone depletion potential Zero
Global warming potential Low
Hazardous air pollutant No
VOC 760 g/L
SARA Not regulated
NESHAPs Not regulated
RCRA Regulated
Storage and packaging

Available in 31 lb (14 kg) pails and 348 lb (158 kg) drums. Shelf life is 36 months when stored in the original sealed container above 10°C (50°F). Listed NSNs include 6850-01-474-2302, 6850-01-474-2309, 6850-01-474-2313, and 6850-01-163-1888. Consult the current Safety Data Sheet for handling and disposal requirements.

Next steps

Evaluate AXAREL™ 1000 for your cleaning process

Contact Krayden to discuss soils, substrates, manual or immersion cleaning, airless vacuum equipment, approval requirements, packaging, bath management, and cleanliness validation.

Leading Brands Trust in Our Products and Services