ARALDITE MY790-1

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

ARALDITE MY790-1

Main features

  • Low-Viscosity Impregnation Processing
  • Long-Pot-Life Bath Stability
  • Solvent-Free Electrical Insulation

Product Description

ARALDITE MY 790-1 Epoxy Resin is a liquid Bis-A epoxy resin component for the hot-curing ARADUR HY 1102 electrical impregnation system. The complete resin and anhydride-hardener formulation is solvent-free and is used for full-bath impregnation and vacuum-pressure impregnation of electric motors, generators, and single conductors with accelerator-containing mica tapes. The reactive mix combines low viscosity, long pot life, and bath stability at elevated temperatures for controlled impregnation processing. Heat cure forms the final insulation system, with cured electrical and mechanical properties governed by the resin-to-hardener ratio, accelerator package, specimen, and cure schedule. MY 790-0.625remains the separately supplied resin component.

Key features

  • Low-viscosity reactive mix: The MY 790-1/HY 1102 system supports impregnation flow at elevated processing temperatures.
  • Long-pot-life bath stability: The specified formulation maintains a stable impregnation bath, including elevated-temperature operation.
  • Solvent-free heat-cure system: The complete epoxy and anhydride-hardener system cures by heat.

Applications

Full-bath and vacuum-pressure impregnation of electric motors, generators, and single conductors used with accelerator-containing mica tapes.

Technical Specifications

General Properties
Color
The color
Gardner <1
Component System
Describes the number of components that must be supplied, mixed, or activated before application or cure.
Two
Density (g)
1.15-1.20 g/cm3
Vapor Pressure
<10^-3 kg/cm2
Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
>200 °C
Chemical Properties
Melting Point
50-55

Leading Brands Trust in Our Products and Services