ARALDITE HARDENER 8579

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

ARALDITE HARDENER 8579

Main features

  • Paste Hardener Formulation
  • Easy to Mix and Apply
  • High-Viscosity Placement Control

Product Description

Hardener 8579 US is a gray paste epoxy curing agent used as the hardener component in the ARALDITE® 8579 adhesive system. The material is supplied as a high-viscosity paste with a specific gravity of 1.71 and is designed for mixing with compatible epoxy resin components. Hardener 8579 is supplied for professional and industrial use and should be handled in accordance with applicable safety requirements. The product is provided in paste form and is intended for use as a reactive hardener in epoxy adhesive formulations.

Key features

  • Paste hardener formulation: Supplied as a gray paste suitable for incorporation into epoxy adhesive systems.
  • Specific gravity of 1.71: Typical density value reported for the hardener component.
  • High-viscosity material: Typical viscosity of 60,000 cP at 25°C.

Technical Specifications

General Properties
Color
The color
Gray
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.71
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
60,000 mPa.s

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties for Hardener 8579 as supplied.

Property Value Unit Method / condition
Appearance Gray paste — Visual appearance
Specific Gravity 1.71 — ASTM D-792
Viscosity 60,000 cP ASTM D-2393 at 25°C
Relative Density 1.6 — SDS value
Flash Point >94 °C Closed cup

 