ARALDITE CW 229

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

ARALDITE CW229

Main features

  • Filled Epoxy Resin
  • High-Viscosity Resin Handling
  • Electrical-Insulation Resin Applications

Product Description

Araldite® CW 229 US Resin is a filled epoxy resin supplied as a beige viscous liquid for use in electrical insulation casting systems. The resin contains mechanically reinforcing fillers and is designed for processing into electrical insulation components used in indoor medium- and high-voltage applications, including SF6-insulated equipment when used as part of the designated curing system. The material is supplied in a high-viscosity liquid form suitable for conventional casting and Automatic Pressure Gelation (APG) processing methods. Araldite® CW 229 US Resin is intended for manufacturers requiring a filled epoxy resin for electrical insulation and encapsulation applications.

Key features

  • Filled epoxy resin formulation: Contains mechanically reinforcing fillers for electrical insulation casting applications.
  • High-viscosity liquid: Supplied as a beige viscous liquid with a viscosity of 80,000-200,000 cP at 25°C.
  • Electrical insulation applications: Intended for electrical insulation components used in medium- and high-voltage equipment.

Applications / Suitable for

  • Electrical insulation castings
  • Electrical insulation components
  • Indoor medium-voltage equipment
  • Indoor high-voltage equipment
  • SF6-insulated electrical equipment
  • Epoxy casting and encapsulation systems

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Beige viscous liquid
Density (g)
1.76 - 1.83 g/cm3
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
80,000 - 200,000 mPa.s
Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
135 °C

Additional Information

Potting, Encapsulation & Electrical Casting

Heat-curing epoxy casting system for electrical insulation

ARALDITE CW 229 resin and ARADUR HW 229-1 hardener form a filled, heat-curing two-component epoxy casting system for electrically insulating components. The exact pair is documented for conventional casting and Automatic Pressure Gelation. The mixed viscosity is temperature-dependent, and the cure schedule is selected according to part mass, mold temperature, and processing method.

100:100 by weight100:90 by volumeAPG compatibleTg 110-120 deg CThermal Index 200 deg C

As supplied

Component properties

Resin and hardener values are shown separately before mixing.

Property ARALDITE CW 229 resin ARADUR HW 229-1 hardener
Appearance Beige viscous liquid Beige viscous liquid
Density 1.76-1.83 g/cm3 1.90-1.98 g/cm3
Viscosity at 25 deg C 80,000-200,000 cP 25,000-75,000 cP
Flash point, closed cup 135 deg C 140 deg C

Properties are based on Huntsman test methods.

Processing

Select the cure profile for the casting size and process

Processing guidance differs for smaller parts, very large parts, and APG casting. The mixed material becomes substantially less viscous as temperature rises.

  1. Mix ARALDITE CW 229 resin and ARADUR HW 229-1 hardener at 100:100 by weight or 100:90 by volume.
  2. For smaller parts, preheat the mold to 80-100 deg C, mix at 40-80 deg C, then gel for 4-6 hours at 80 deg C or 2 hours at 100 deg C before the stated post-cure.
  3. For very large parts, use a step or ramp cure; one example ramps from 60-80 deg C to 140 deg C over 16-24 hours, followed by 4-6 hours at 140 deg C and slow cooling before demolding.
  4. For APG, preheat the mold to 140-160 deg C, fill in 2-5 minutes with mixed material at 50-60 deg C, and gel under 1-3 atm for 7-15 minutes before the stated post-cure.
  5. Typical mixed viscosity is 35,000-65,000 cP at 25 deg C, 2,500-3,500 cP at 50 deg C, and 700-1,200 cP at 70 deg C.

Storage and handling

Keep filled components dry and homogenized before processing

Store both components in dry, sealed original containers at 2-40 deg C. Under these conditions, shelf life is 1 year from date of manufacture.

The hardener is moisture-sensitive after opening. Reseal immediately and use nitrogen blanketing or desiccant venting when material will not be used rapidly.

Because the components are prefilled, carefully homogenize them with a low-shear mixer before processing and take precautions to avoid air entrapment.

Cured system

Typical cured physical and electrical properties

These values apply to the cured ARALDITE CW 229 / ARADUR HW 229-1 system and are not properties of the hardener alone.

Property Typical value Method
Tensile strength 11,000-12,500 psi ASTM D638
Flexural strength 18,000-19,000 psi ASTM D790
Hardness Shore D 92-96 Shore D
Glass transition temperature 110-120 deg C DSC
Thermal conductivity 0.7-0.8 W/m-K ISO 8894-2/90
Dielectric strength 420-480 V/mil at 3 mm IEC 60243
Critical stress intensity factor, K1C 2.8-3.0 MPa-m^0.5 Double Torsion Test

Unless otherwise stated, these are typical values and not a product specification.

Applications

Supported applications

Use the documented application scope below as the starting point for product evaluation.

Electrical insulating components

Casting of electrically insulating components where the documented CW 229 / HW 229-1 system and cure process are appropriate.

Medium-voltage insulation

Indoor medium-voltage electrical insulation applications within the exact system's documented processing and qualification scope.

High-voltage and SF6 insulation

Indoor high-voltage applications, including SF6-insulated types, as documented for the complete system.

Technical support for ARALDITE CW 229 / ARADUR HW 229-1

Need help matching the CW 229 / HW 229-1 system to casting geometry, APG conditions, cure schedule, or electrical-property requirements? Krayden can help review the exact component pairing, processing temperatures, part mass, and qualification needs before the system is evaluated in the intended electrical assembly.

Contact Us