ARALDITE AW 8595

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

ARALDITE AW8595

Main features

  • 1:1 mix ratio
  • Room temperature curing
  • Strong curing mechanical properties

Product Description

ARALDITE® AW 8595 / HARDENER HW 8595 Epoxy Adhesive System is a two-component epoxy adhesive system from Huntsman Advanced Materials designed for metal bonding and other structural bonding applications. The system combines ARALDITE® AW 8595 resin with HARDENER HW 8595 at a 1:1 mix ratio by volume, providing convenient processing and room-temperature cure capability. Typical mixed material properties include a 60-minute pot life at 25°C and a mixed viscosity of approximately 21,000 cP. After cure, the adhesive develops strong mechanical performance, including typical lap shear strength of 2,600 psi (17.9 MPa), Shore D hardness of 70, and tensile strength of 2,200 psi (15.1 MPa), making it suitable for evaluation in metal assembly and general industrial bonding applications.

Key features

  • 1:1 mix ratio by volume: Supports straightforward mixing and application for industrial bonding processes.
  • Room-temperature curing: Provides handling strength after approximately 4 hours at 25°C without elevated-temperature cure requirements.
  • Strong cured mechanical properties: Develops typical lap shear strength of 2,600 psi (17.9 MPa) and Shore D hardness of 70 after full cure.

Applications / Suitable for

  • Metal-to-metal bonding
  • Industrial assembly applications
  • General structural bonding of metal substrates
  • Applications requiring room-temperature cure capability

Technical Specifications

General Properties
Color
The color
Cream
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.23
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
33000 mPa.s
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
30 %
Thermal Properties
Glass Transition Temperature (Tg)
The glass transition temperature for organic adhesives is a temperature region where the polymers change from glassy and brittle to soft and rubbery. Increasing the temperature further continues the softening process as the viscosity drops too. Temperatures between the glass transition temperature and below the decomposition point of the adhesive are the best region for bonding. The glass-transition temperature Tg of a material characterizes the range of temperatures over which this glass transition occurs.
61 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical processing and handling properties for the resin, hardener, and mixed adhesive system.

Property Value Unit Method / condition
Mix Ratio (Resin:Hardener) 100:100 volume Typical mixed system
Mix Ratio (Resin:Hardener) 100:77 weight Typical mixed system
Pot Life 60 min 100 g mass at 25°C
Mixed Viscosity 21,000 cP At 25°C
Resin Specific Gravity 1.23 - ARALDITE® AW 8595, 25°C
Hardener Specific Gravity 0.94 - HARDENER HW 8595
Technical properties

After-processing / final-state properties

Typical cured properties after 7 days at 25°C unless otherwise noted.

Property Value Unit Method / condition
Lap Shear Strength 2,600 (17.9) psi (MPa) ASTM D1002, tested at 25°C
Hardness 70 Shore D ASTM D2240
Ultimate Tensile Strength 2,200 (15.1) psi (MPa) ASTM D638
Ultimate Elongation 30 % ASTM D638
Glass Transition Temperature (Tg) 61 (141) °C (°F) ASTM D4065, DMA