ARALDITE 5864

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

ARALDITE 5864

Main features

  • Up to 5 mm Gap Filling
  • 16.5 MPa Aluminum Lap Shear
  • UL-Recognized 180 deg C Insulation Component

Product Description

ARALDITE® 5864 A/B is a two-component, thixotropic, room-temperature-curing epoxy paste for bonding metals, ceramics, glass-reinforced plastic (GRP) structures and electronic components. The resin and hardener mix 100:50 by weight or volume to form a black paste with a typical 40-minute pot life for a 4 fl oz mass at 25°C. Its non-sag consistency supports gap filling up to 5 mm, while a recommended 0.05–0.10 mm bondline is used where maximum lap shear strength is required. Published data includes typical aluminum lap shear strength of 16.5 MPa after seven days at 25°C, electrical insulation properties, and bonded-joint testing after temperature, humidity, water and chemical exposure. The product is a UL®-recognized system component in the 180°C class for electrical insulation systems.

Key features

  • Controlled paste application: Thixotropic, non-sag mixed adhesive fills gaps up to 5 mm and provides a typical 40-minute pot life at 25°C.
  • Documented bonded-joint performance: Typical aluminum lap shear strength reaches 16.5 MPa after seven days at 25°C, with additional metal, temperature and environmental exposure data.
  • Electrical insulation scope: Published dielectric properties and UL® recognition as a system component in the 180°C electrical insulation class support evaluation for electrical assemblies.

Applications / Suitable for

  • Electronic component bonding
  • GRP structures and assemblies
  • Metal and ceramic bonding where water, chemicals or elevated temperatures may be encountered

Technical Specifications

General Properties
Color
The color
Black
Density (g)
1.6 g/cm3
Pot Life
Pot life is the amount of time it takes for the viscosity of a material to double (or quadruple for lower viscosity materials) in room temperature after a material is mixed. It is closely related to work life but it is not application dependent, less precise and more of a general indication of how fast a system is going to cure.
40 minutes
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
90000 mPa.s
Viscosity (Part A)
70000 mPa.s
Viscosity (Part B)
130000 mPa.s

Additional Information

Technical properties

As-supplied / before-processing properties

Typical resin, hardener and mixed-system data. Values are technical information rather than guaranteed production specifications.

Property Value Unit Method / condition
Product form Two-component thixotropic epoxy paste — Room-temperature curing
Appearance Resin A: beige paste; Hardener B: black thixotropic paste; mixed system: black paste — Visual
Mix ratio 100:50 (2:1) parts Resin A:Hardener B; by weight and by volume
Density Resin A: 1.60; Hardener B: 1.60 g/cm³ Typical at 25°C; ASTM D792
Viscosity Resin A: 70,000; Hardener B: 130,000; mixed system: 90,000 cP Typical at 25°C; ASTM D2393
Pot life 40 minutes Typical for a 4 fl oz mixed mass at 25°C; ASTM D2471
Non-sag gap filling Up to 5 (0.2) mm (in) Thixotropic mixed paste
Technical properties

After-processing / final-state properties

Typical cured-adhesive and bonded-joint data under the stated cure, substrate and test conditions. These values are not universal design allowables.

Property Value Unit Method / condition
Lap shear strength 16.5 (2400) MPa (psi) Typical; aluminum lap joint; cure 7 days at 25°C; DIN 53283
Lap shear strength with post-cure 17.9 (2600) MPa (psi) Typical; aluminum lap joint; cure 24 h at 25°C plus 30 min at 80°C; DIN 53283
Lap shear strength on stainless steel 22 (3200) MPa (psi) Typical; 1.0 mm stainless steel; cure 16 h at 40°C; DIN 53283
Glass transition temperature, Tg 110 (230) °C (°F) Typical; DMA; ASTM D4065
Hardness 84 Shore D Typical cured adhesive
Roller peel 3 (17) N/mm (pli) Typical; ISO 4578
Dielectric strength 440 V/mil Typical electrical property
Volume resistivity 6.1 × 1015 Ω·cm Typical electrical property