ARALDITE 2051

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

ARALDITE 2051

Main features

  • Rapid 15-Minute Strength Development
  • 1:1 Non-Sag Cartridge Processing
  • 20 MPa structural Lap Shear

Product Description

ARALDITE® 2051 is a fast-curing, two-component toughened methacrylate structural adhesive for metal, plastic and composite bonding. It mixes 1:1 by weight or volume, forms a non-sagging pale-yellow adhesive and provides a 4–6 minute pot life for a 20 g mass at 25°C. The system can be applied and cured from 0°C to 40°C, including humid conditions and underwater. Specified lap shear strength exceeds 20 MPa at 25°C, while typical cured properties include 40 MPa tensile strength, 1700 MPa tensile modulus and approximately 10% elongation at break. Surface cleaning is recommended, with abrasion or chemical etching used where maximum joint durability is required.

Key features

  • Fast strength development from 0°C to 40°C: On sandblasted aluminium under contact pressure, typical lap shear exceeds 1 MPa after 15 minutes and 10 MPa after 25 minutes at 23°C.
  • Wet and humid-area processing: Supports application and cure in humid environments and underwater.
  • Toughened structural performance: Specified lap shear strength is above 20 MPa at 25°C, with service-temperature suitability documented up to 120°C.

Applications / Suitable for

  • Structural bonding of aluminium, steel, stainless steel and galvanised steel
  • Selected plastics and composites, including CFRP, GRP, PMMA, PVC, polycarbonate and ABS
  • Bonding operations in humid or underwater conditions

Technical Specifications

General Properties
Color
The color
Yellow
Pot Life
Pot life is the amount of time it takes for the viscosity of a material to double (or quadruple for lower viscosity materials) in room temperature after a material is mixed. It is closely related to work life but it is not application dependent, less precise and more of a general indication of how fast a system is going to cure.
5 minutes
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1
Physical Properties
Viscosity (Part A)
48000 mPa.s
Viscosity (Part B)
22500 mPa.s

Additional Information

Technical properties

As-supplied / before-processing properties

Values distinguish the resin, hardener and mixed adhesive where applicable. Specified values retain the stated test mass, temperature and method context.

Property Value Unit Method / condition
Colour Off-white / yellow-greenish / pale yellow — Resin / hardener / mixed adhesive; visual
Specific gravity ca. 1 / ca. 1 / ca. 1 — Resin / hardener / mixed adhesive
Viscosity at 25°C 35–60 / 15–30 Pa·s Resin / hardener
Mixed-adhesive rheology Non-sagging — Mixed adhesive at 25°C
Mix ratio by weight 100:100 parts Resin : hardener
Mix ratio by volume 100:100 parts Resin : hardener
Pot life 4–6 min 20 g mixed mass at 25°C; specified
Time to peak exotherm 8–14 min 20 g mixed mass; method A159; specified
Technical properties

After-processing / final-state properties

The lap shear value is specified. Other values are typical laboratory data and must not be treated as guaranteed design values for every substrate, joint or service condition.

Property Value Unit Method / condition
Lap shear strength at 25°C >20 MPa Mixed adhesive; method A501; specified
Glass transition temperature, onset 98 °C Typical average; DMA; cure 24 h at room temperature
Glass transition temperature, midpoint 127 °C Typical average; DMA; cure 24 h at room temperature
Tensile strength 40 MPa Typical average; ISO 527; cure 24 h at room temperature; tested at 23°C
Tensile modulus 1700 MPa Typical average; ISO 527; cure 24 h at room temperature; tested at 23°C
Elongation at break ca. 10 % Typical average; ISO 527; cure 24 h at room temperature; tested at 23°C
Service temperature capability Up to 120 °C Documented product key property; validate the bonded assembly under actual service conditions