ARALDITE 2021-1

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

ARALDITE 2021-1

Main features

  • Rapid 9-Minute Strength Development
  • Broad Multi-Material Bonding
  • 27 MPa Aluminum Lap Shear

Product Description

ARALDITE® 2021-1 is a two-component, room-temperature-curing, toughened methacrylate structural adhesive for rapid assembly of selected plastics, composites and metals. The 1:1 mix system forms a thixotropic, pale-yellow adhesive with a typical pot life of approximately 3 minutes at 25°C. It can be dispensed manually or robotically, including from mixer-equipped cartridges. A typical 0.25-0.5 mm adhesive layer is recommended for high lap-shear performance, although some steel joints may require greater thickness. The cured adhesive is suitable for service temperatures up to 100°C. It should not be selected for copper, brass or copper-alloy substrates.

Key features

  • Rapid strength development: Typical lap shear strength exceeds 1 MPa after 9 minutes and 10 MPa after 13 minutes at 23°C.
  • Multi-material bonding: Supports bonding of selected plastics, composites and metals, with substrate-specific testing reported for multiple grades.
  • Toughened cured performance: Typical tensile strength is 42 MPa with elongation above 10%, and service use is supported up to 100°C.

Applications / Suitable for

  • Rapid assembly operations using manual or robotic adhesive application
  • Bonding selected plastics and composites, including GRP, CFRP, SMC, ABS, PVC, PMMA, PC and polyamides
  • Bonding aluminium, mild steel, stainless steel and galvanised steel

Technical Specifications

General Properties
Pot Life
Pot life is the amount of time it takes for the viscosity of a material to double (or quadruple for lower viscosity materials) in room temperature after a material is mixed. It is closely related to work life but it is not application dependent, less precise and more of a general indication of how fast a system is going to cure.
3 minutes
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1
Physical Properties
Viscosity (Part A)
32000 mPa.s
Viscosity (Part B)
30000 mPa.s

Additional Information

Technical properties

As-supplied and mixed properties

Specified and typical product data are shown with the applicable component or mixed state. Typical values are not guaranteed specifications.

Property Value Unit Method / condition
Part A colour Off-white - Visual
Part B colour Yellow / greenish - Visual
Mixed adhesive colour Pale yellow - Visual
Specific gravity A: 1.02; B: 0.95; mixed: approx. 1 - Component and mixed-material values
Component viscosity A: 15-50; B: 10-50 Pa·s 25°C; method A191
Mixed adhesive rheology Thixotropic - Mixed state
Mix ratio 100:100 parts By weight and by volume
Pot life Approx. 3 min 100 g mixed adhesive at 25°C
Time to peak exotherm 7-15 min 20 g mixed adhesive; method A159
Cured adhesive performance

Typical final-state properties

Typical laboratory data are provided for technical evaluation and are not guaranteed specifications. Cure and test conditions are retained where they affect interpretation.

Property Value Unit Method / condition
Tensile strength 42 MPa Typical; ISO 527; cured 16 h at 40°C and tested at 23°C
Tensile modulus 1800 MPa Typical; ISO 527; cured 16 h at 40°C and tested at 23°C
Elongation at break >10 % Typical; ISO 527; cured 16 h at 40°C and tested at 23°C
Time to lap shear strength >1 MPa 9 min Typical at 23°C
Time to lap shear strength >10 MPa 13 min Typical at 23°C
Service temperature Up to 100 °C Supplier key property; validate in the intended joint and service environment
Lap shear after thermal cycling 27 MPa Typical; ISO 4587 on aluminium; sandblasted and degreased; cured 16 h at 40°C; 100 cycles of 6 h from -30°C to 70°C

Technical selection guidance

Surface preparation and joint design
Degreasing is the minimum recommended preparation. Mechanical abrasion or chemical etching after degreasing supports stronger and more durable joints. Avoid low-grade alcohol, gasoline and paint thinners. Validate bondline thickness and fixation using the actual substrate pair and joint geometry.
Substrate scope and limitations
The product is not suitable for copper, brass or copper-alloy substrates. Under the reported ISO 4587 plastic-joint test conditions, substrate failure was observed for EP-GRP, UP-GRP, ABS, PVC, PMMA and PC. Bond performance remains specific to the substrate grade, surface preparation, cure and joint configuration.