ARALDITE 2014-2

Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics

ARALDITE 2014-2

Main features

  • 110-Minute Pot Life
  • Non-Sagging Five-Millimeter Gap Fill
  • High Chemical and Water Resistance

Product Description

ARALDITE 2014-2 A/B Structural Adhesive is a two-component, room-temperature-curing thixotropic epoxy paste adhesive for structural bonding. The complete system combines Part A resin and Part B hardener at 100:50 by weight or volume, producing a grey mixed paste with a typical 110-minute pot life for 100 g at 25 deg C. It is non-sagging in gaps up to 5 mm and is designed for high strength with good environmental and chemical resistance. The adhesive is documented for metals, electronic components, and GRP structures where elevated service temperature or aggressive exposure is expected. Typical cured data include 60 MPa flexural strength and 30 MPa tensile strength after 16 hours at 40 deg C, tested at 23 deg C.

Key features

  • Long controlled working time: The mixed system has a typical 110-minute pot life for 100 g at 25 deg C.
  • Gap-filling thixotropy: The paste remains non-sagging in bond gaps up to 5 mm.
  • Chemically resistant cured system: Documented performance supports demanding structural-bonding environments.

Applications

Structural bonding of metals, electronic components, and GRP structures in demanding service environments.

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
grey paste
Mix Ratio
The amount of a constituent divided by the total amount of all other constituents in a mixture
100:50
Pot Life
Pot life is the amount of time it takes for the viscosity of a material to double (or quadruple for lower viscosity materials) in room temperature after a material is mixed. It is closely related to work life but it is not application dependent, less precise and more of a general indication of how fast a system is going to cure.
110 minutes

Additional Information

Technical properties

As-supplied / before-processing properties

Component and mixed-state data are identified separately; values are approximate or typical as stated.

PropertyValueUnitMethod / condition
Part A appearanceBeige pasteVisual; A112
Part B appearanceGrey pasteVisual; A112
Mixed appearanceGrey pasteVisual; A112
Part A specific gravityApprox. 1.6As supplied
Part B specific gravityApprox. 1.5As supplied
Part A viscosity50-80Pa.s25 deg C
Mix ratio, A:B100:50partsBy weight or by volume
Mixed pot life110minutes100 g at 25 deg C
Technical properties

After-processing / final-state properties

Typical cured-system values. Cure and test conditions remain attached to each result.

PropertyValueUnitMethod / condition
Glass-transition temperatureApprox. 69deg CDMA; cured 16 hours at 40 deg C
Glass-transition temperatureApprox. 85deg CDSC; cured 24 hours at 23 deg C plus 1 hour at 80 deg C
Flexural strength60MPaISO 178; cured 16 hours at 40 deg C; tested at 23 deg C
Flexural modulus3,500MPaISO 178; cured 16 hours at 40 deg C; tested at 23 deg C
Tensile strength30MPaISO 527; cured 16 hours at 40 deg C; tested at 23 deg C
Tensile modulus3,100MPaISO 527; cured 16 hours at 40 deg C; tested at 23 deg C
Elongation at break0.9%ISO 527; cured 16 hours at 40 deg C; tested at 23 deg C
Dielectric strength25kV/mmASTM D-149; typical