ARALDITE 2013-1

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

ARALDITE 2013-1

Main features

  • Thixotropic Vertical-Surface Control
  • 80 to 90-Minute Working Window
  • 17 MPa Lap Shear

Product Description

ARALDITE® 2013-1 is a two-component, room-temperature-curing epoxy paste adhesive developed primarily for metal bonding and also suitable for ceramics, glass, rubbers, rigid plastics, and other commonly used materials. Its thixotropic, metal-colored paste supports vertical application and mixes at 100:60 by weight or 1:1 by volume. The mixed adhesive has a pot life of 80–90 minutes for a 100 g mass at 25°C, providing a practical assembly window. A 0.05–0.10 mm adhesive layer is recommended for greatest lap shear strength, with specified lap shear strength above 17 MPa at 23°C. The cured system combines high strength and toughness with documented environmental and chemical resistance.

Key features

  • Vertical-application paste: Thixotropic rheology supports application on vertical joint surfaces.
  • Controlled mixing and working time: Mixes 1:1 by volume and provides an 80–90 minute pot life for 100 g at 25°C.
  • Documented strength and resistance: Specified lap shear strength exceeds 17 MPa at 23°C, with documented environmental and chemical resistance.

Applications / Suitable for

  • Metal bonding
  • Ceramic and glass bonding
  • Rubber and rigid-plastic bonding

Technical Specifications

General Properties
Pot Life
Pot life is the amount of time it takes for the viscosity of a material to double (or quadruple for lower viscosity materials) in room temperature after a material is mixed. It is closely related to work life but it is not application dependent, less precise and more of a general indication of how fast a system is going to cure.
85 minutes
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.2
Physical Properties
Viscosity (Part A)
550000 mPa.s

Additional Information

Technical properties

As-supplied / before-processing properties

Component and mixed-material properties for ARALDITE® 2013-1. Preserve the stated component, quantity, temperature, and ratio basis when evaluating processing.

Property Value Unit Method / condition
Part A appearance Grey paste — Visual method A112; specified data
Part B appearance Beige paste — Visual method A112; specified data
Mixed appearance Grey paste — Visual method A112; specified data
Specific gravity A: ca. 1.4; B: ca. 0.9; mixed: ca. 1.2 — As supplied
Part A viscosity 380–720 Pa·s At 25°C
Part B and mixed rheology Thixotropic — At 25°C
Pot life 80–90 min 100 g mixed mass at 25°C
Mix ratio, A:B 100:60 by weight; 1:1 by volume — Bulk mixing or cartridge format
Technical properties

After-processing / final-state properties

Cured-property values are tied to the stated methods and cure conditions. Typical averages are technical information, not guaranteed design values.

Property Value Unit Method / condition
Lap shear strength >17 MPa At 23°C; method A501; specified data
Tensile strength 22 MPa ISO 527; cure 16 h at 40°C; tested at 23°C; typical average
Tensile modulus 1370 MPa ISO 527; cure 16 h at 40°C; tested at 23°C; typical average
Elongation at break 1.8 % ISO 527; cure 16 h at 40°C; tested at 23°C; typical average
Glass transition temperature 63.3 °C DMA; cure 16 h at 40°C; typical average