ARADUR HY 918

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

ARADUR HY 918

Main features

  • 50-80 mPa.s Component Viscosity
  • APG or Vacuum-Casting Processing
  • High-Voltage Insulation System Use

Product Description

ARADUR HY 918 Hardener is represented in the supplied technical document as ARADUR HY 918 CI, a liquid anhydride hardener for a low-viscosity, hot-curing electrical casting system based on ARALDITE CY 228 CI. As supplied, the CI component has guideline viscosity of 50-80 mPa.s and density of 1.18-1.24 g/cm3 at 25 deg C, with an approximate 165 deg C flash point. The documented formulation uses 85 parts hardener per 100 parts resin by weight, with optional flexibilizer, accelerator, and silica filler. It supports automatic pressure gelation or conventional vacuum casting for medium- and high-voltage indoor electrical insulators. Cured performance remains specific to the complete formulation and stated cure conditions.

Key features

  • Low component viscosity: Guideline viscosity is 50-80 mPa.s at 25 deg C.
  • Two documented casting routes: The CY 228 CI system supports automatic pressure gelation or conventional vacuum casting.
  • High-voltage system use: The documented formulation is intended for medium- and high-voltage indoor electrical insulators.

Applications

As the HY 918 CI hardener component in CY 228 CI formulations for switch and apparatus components, pin insulators, bushings, and power-distribution, current, or voltage transformers.

Technical Specifications

Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
50-80 mPa.s
General Properties
Density
Volumetric mass per unit
1.18-1.24 kg/m3
Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
165 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Guideline values for the ARADUR HY 918 CI component named in the supplied TDS; cured-system data are excluded.

PropertyValueUnitMethod / condition
Viscosity50-80mPa.s25 deg C; DIN 53015
Density1.18-1.24g/cm325 deg C; ISO 1675
Flash pointApprox. 165deg CDIN 51758
Vapor pressureApprox. 1mbar25 deg C; Knudsen
Vapor pressureApprox. 10mbar60 deg C; Knudsen