ALPHA WS826

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

ALPHA WS826

Main features

  • Eight-Hour High-Humidity Stencil Life
  • Air or Nitrogen Reflow
  • Zero-Halogen Water-Soluble Flux

Product Description

ALPHA WS-826 Solder Paste is a water-soluble, lead-free, zero-halogen solder paste developed for SAC305 assembly in air or nitrogen reflow. Type 4 and Type 5 powder options support fine-pitch printing, while the formulation maintains an eight-hour stencil life at both 25 deg C/50% RH and 30 deg C/70% RH. Its flux is classified ORM0 to IPC J-STD-004B, with no halides or halogens detected by the cited methods. Cold- and hot-slump testing passed without bridging above 0.20 mm and 0.25 mm, respectively. Residues are designed for hot deionized-water removal in batch or inline equipment after one or two reflow cycles. Properly stored unopened paste has a six-month shelf life at 0-10 deg C.

Key features

  • High-humidity stencil stability: Maintains eight-hour transfer efficiency at 30 deg C and 70% RH.
  • Air or nitrogen reflow: Supports SAC305 processing in either documented atmosphere.
  • Aqueous two-reflow cleanability: Residues are designed for hot deionized-water removal after one or two reflows.

Applications

SAC305 Type 4 or Type 5 SMT printing and air or nitrogen reflow with batch or inline aqueous cleaning.

Product Family

ALPHA WS826

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Alloy Composition
Composition of the alloy material
SAC305

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
AlloySAC305Available configuration
Powder sizesType 4; Type 5Available configurations
Flux classificationORM0IPC J-STD-004B
Halide / halogen contentNone detectedIPC J-STD-004B / BS EN 14582
Tack lifeConsistent over 24hoursJIS Z 3284
Ambient stencil life8hours25 deg C, 50% RH
Elevated-condition stencil life8hours30 deg C, 70% RH
Shelf life6monthsUnopened, refrigerated at 0-10 deg C