ALPHA WS809

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

ALPHA WS809

Main features

  • Print Speeds From 1 to 6 Inches
  • Eight-Hour Stencil Life
  • Water-Cleanable After Two Reflows

Product Description

ALPHA WS-809 Solder Paste is a water-soluble tin-lead solder paste for a broad range of stencil-printed SMT processes using aqueous post-reflow cleaning. It supports fine-pitch printing, including 0.016 in pitch QFP patterns and 0.015 in circular apertures, at print speeds from 1 to 6 in/s. Available alloy options include 63Sn/37Pb, 62Sn/36Pb/2Ag, and NT4S, with 89.8% metal loading in Type 3 or Type 4 powder. Typical physical data include 4.4 g/cc paste density for 63Sn/37Pb, 1,550 to 2,550 poise viscosity at 10 rpm, and eight hours of stencil life at 24-27 deg C and 30-50% RH. Residues remain water-cleanable after two reflow cycles.

Key features

  • Broad print-speed range: Supports stencil printing from 1 to 6 in/s under the documented process.
  • Eight-hour stencil life: Maintains stencil performance at 24-27 deg C and 30-50% RH.
  • Two-reflow cleanability: Flux residues remain water-cleanable after two paste reflow cycles.

Applications

Fine-pitch and general stencil-printed SMT assembly using tin-lead alloys and aqueous post-reflow cleaning.

Product Family

ALPHA WS809

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Alloy Composition
Composition of the alloy material
Sn63/Pb37; Sn62/Pb36/Ag2; NT4S

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
Alloy options63Sn/37Pb; 62Sn/36Pb/2Ag; NT4SAvailable configurations
Metal loading89.8%Typical configuration
Powder sizesType 3: 25-45 um; Type 4: 20-38 umIPC J-STD-005
Flux activityORH0IPC J-STD-004A
Paste density4.4g/ccTypical; 63Sn/37Pb alloy
Viscosity1,550-2,550PoiseMalcom spiral viscometer, ICP-029, 10 rpm
Stencil life8hours24-27 deg C, 30-50% RH
Shelf life6monthsRefrigerated at 0-10 deg C

Leading Brands Trust in Our Products and Services