Main features

  • 0.008-Inch Fine-Pitch Printing
  • Over Four Hours Stencil Life
  • Completely Water-Soluble Flux

Product Description

ALPHA WS-619 Solder Paste is a completely water-soluble, halide-free solder paste for stencil-applied surface-mount assembly where aqueous post-reflow cleaning is required. It supports standard and fine-pitch printing through apertures as small as 0.008 in (0.2 mm) and produces repeatable deposits on 0.016 in (0.4 mm) pitch pads. The paste is offered with 63Sn/37Pb, 62Sn/36Pb/2Ag, and SAC305 alloys in Type 3 or Type 4 powder. Its ORH0 flux carries 0% halide by titration. Typical process data include more than four hours of stencil life at 50% RH and 72 deg F and tack force above 1.5 g/mm2 at six hours. Unopened refrigerated paste has a nominal three-month shelf life between 0 and 10 deg C.

Key features

  • Fine-pitch print capability: Supports stencil apertures down to 0.008 in under the documented process.
  • Sustained stencil performance: Stencil life exceeds four hours at 50% RH and 72 deg F.
  • Completely water-soluble residues: The flux system is designed for aqueous cleaning after reflow.

Applications

Standard and fine-pitch stencil printing for SMT assemblies that use aqueous post-reflow cleaning.

Product Family

ALPHA WS619

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Alloy Composition
Composition of the alloy material
Sn63/Pb37; Sn62/Pb36/Ag2; SAC305

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
Alloy options63Sn/37Pb; 62Sn/36Pb/2Ag; SAC305Available configurations
Powder sizesType 3; Type 4Available configurations
Packaging500 g jars; 6 in and 12 in cartridges; 10 cc and 30 cc syringesAvailable formats
Flux designationORH0IPC J-STD-004
Halide content0%By titration
Tack force> 1.5g/mm2At 6 hours; J-STD-005
Stencil life> 4hours50% RH, 72 deg F
Shelf life3monthsRefrigerated at 0-10 deg C