ALPHA WS609

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

ALPHA WS609

Main features

  • Four-Hour Stencil Life
  • Complete Water-Cleanable Residue Removal
  • Type 3 to 5 Powders

Product Description

ALPHA WS-609 Solder Paste is a halide-free, neutral-pH water-soluble solder paste for stencil-printed surface-mount assembly and other processes that use post-reflow water cleaning. Its water-soluble carrier supports complete residue removal, while the activator system is designed to wet tarnished surfaces across documented base metals and finishes. Type 3 and Type 4 powders support printing; Type 5 is available for dispensing applications, with several tin-lead and lead-free alloy options. Stencil life is four hours and tack life exceeds six hours at 21-27 deg C and 30-60% RH. Nominal spiral viscosity is 3,000 poise at 5 rpm, and refrigerated shelf life is three months at 0-10 deg C.

Key features

  • Controlled print window: Four-hour stencil life supports stable surface-mount printing.
  • Extended component-placement time: Tack life exceeds six hours under the stated temperature and humidity range.
  • Complete residue cleanability: Flux residues are designed for removal with hot water after reflow.

Applications

Stencil printing, dispensing, and demanding electronics assembly processes that use post-reflow water cleaning.

Product Family

ALPHA WS609

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Alloy Composition
Composition of the alloy material
Sn63/Pb37; Sn95/Sb5; Sn62/Pb36/Ag2; Sn99.3/Cu0.7; SAC305

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
Alloy options63Sn37Pb; 95Sn5Sb; 62Sn36Pb2Ag; 99.3Sn0.7Cu; SAC305Available configurations
Powder sizesType 3; Type 4; Type 5 for dispensingAvailable configurations
Water-extract resistivity> 100,000ohm-cmTypical
Halide contentHalide-freeChemical property
Flux-residue pH6.8Typical
Nominal viscosity3,000PoiseSpiral viscometry, 5 rpm
Stencil life4hours21-27 deg C, 30-60% RH
Shelf life3monthsRefrigerated at 0-10 deg C