ALPHA WS362

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

ALPHA WS362

Main features

  • High-activity, 25% solids water-soluble flux designed for densely packed assemblies and multilayer boards requiring relatively high preheat temperatures.
  • Highly water-soluble post-solder residues support effective cleaning for high ionic cleanliness and surface insulation resistance.
  • Halide-free formulation with rapid wetting and support for foam, spray, or wave application techniques.

Product Description

ALPHA WS362-25 Water-Soluble Surface Mount Flux is a halide-free, water-soluble organic flux designed for soldering surface mount and mixed technology assemblies where effective residue removal and high ionic cleanliness are important. Its high-activity, 25% solids formulation is recommended for densely packed assemblies and multilayer boards requiring relatively high preheat temperatures. After soldering, the highly water-soluble residues can be readily removed, supporting high ionic cleanliness and surface insulation resistance. ALPHA WS362-25 can be applied by foam, spray, or wave techniques and is designated ORMO according to IPC J-STD-004.

Key features

  • Highly water-soluble residue: Designed for effective post-solder cleaning where high ionic cleanliness is required.
  • High activity and 25% solids: Recommended for densely packed assemblies and multilayer boards requiring relatively high preheat temperatures.
  • Halide-free formulation: Provides rapid wetting and carries an ORMO designation according to IPC J-STD-004.
  • Multiple application methods: Suitable for foam, spray, and wave application techniques.

Applications / Suitable for

  • Surface mount assemblies
  • Mixed technology assemblies
  • Densely packed assemblies requiring effective residue cleaning
  • Multilayer boards requiring relatively high preheat temperatures
Product Family

ALPHA WS362

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Solids
25 %
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
0.846 ± 0.005 @25°C

Additional Information

Technical properties

As-supplied / before-processing properties

Selected typical properties of ALPHA WS362-25 in its as-supplied liquid state.

Property Value Unit Method or condition
Appearance Clear, pale yellow - As supplied
Solids content 25 wt/wt % Typical value
Specific gravity 0.846 +/- 0.005 - 25 °C (77 °F)
Acid number 33.00 +/- 2.00 mg KOH/g Typical value
pH 3.2 - 5% aqueous solution
Flash point 17 °C T.C.C.
Technical properties

After-processing / final-state properties

Surface insulation resistance results for ALPHA WS362-25 after hydrocleaning under the stated IPC J-STD-004 test conditions.

Property Result Requirement Method or condition
Surface insulation resistance - Comb-Down, hydrocleaned 4.4 x 108 ohms >1.0 x 108 ohms IPC J-STD-004; 85 °C/85% RH, 7 days; -50 V, measurement at 100 V on IPC B-24 board
Surface insulation resistance - Control Boards 3.6 x 109 ohms >1.0 x 109 ohms IPC J-STD-004; 85 °C/85% RH, 7 days; -50 V, measurement at 100 V on IPC B-24 board

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers