SnCX Plus 07

Harmonization Code : 8001.20 | Unwrought tin: Tin alloys

SnCX Plus 07

Main features

  • Silver-Free Lead-Free Wave-Soldering Alloy
  • Reduced Copper Dissolution at High Temperature
  • Vaculoy Low-Dross Fast-Wetting Processing

Product Description

ALPHA® SnCX Plus® 07 is a silver-free, lead-free solder alloy for wave soldering, selective soldering, lead tinning, and rework processes. It is designed as an alternative to SnPb, SAC305, and other low-silver SAC alloys and is suitable for through-hole and surface-mount components on single-sided and mixed-technology assemblies. The alloy is engineered to limit copper dissolution, reduce dross generation, and provide fast wetting with smooth, bright solder fillets. Its approximate melting temperature is 227 °C, with a recommended solder-pot operating range of 255 to 270 °C.

Key features

  • Silver-free, lead-free alloy: Designed as an alternative to SnPb, SAC305, and other low-silver SAC solder alloys.
  • Controlled copper erosion: Engineered to minimize copper dissolution during extended high-temperature soldering and rework processes.
  • Low-dross processing: Uses the proprietary Vaculoy® manufacturing process with a dross-reducing addition to limit included oxides and dross generation.

Applications / Suitable for

  • Wave soldering
  • Selective soldering
  • Lead tinning
  • Rework of through-hole and surface-mount components
Product Family

ALPHA SNCX PLUS 07

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

Chemical Properties
Melting Point
227
General Properties
Density (g)
7.30 g/cm3
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
33.1 %

Additional Information

Technical properties

As-supplied / before-processing properties

Typical bulk-alloy and processing properties of ALPHA® SnCX Plus® 07. Typical technical data are not intended for specification purposes.

Property Value Unit Method / condition
Alloy type Silver-free, lead-free solder alloy — Maximum lead content: 0.05%
Melting temperature Approximately 227 °C Typical
Density 7.30 g/cc Typical
Hardness 9.4 HV Test method not stated
Specific heat capacity 0.198 J/g/°C At 100 °C
Thermal expansion coefficient 23.8 µm/m·°C 30 to 100 °C
24.3 µm/m·°C 100 to 180 °C
Tensile stress 42.0 MPa Bulk-alloy value; test method not stated
Yield stress 33.4 MPa Bulk-alloy value; test method not stated
Elongation 33.1 % Bulk-alloy value; test method not stated
Recommended solder-pot temperature 255 to 270 (491 to 518) °C (°F) Wave and selective soldering guidance

Leading Brands Trust in Our Products and Services