ALPHA SM351F

Harmonization Code : 3404.90.00.00 | Artificial waxes and prepared waxes : Other

ALPHA SM351F

Main features

  • Fast-Wetting Foam and Wave Flux
  • Tack-Free Pin-Testable Residue
  • Halide-Free Low-Solids Formulation

Product Description

ALPHA SM-351F Liquid Soldering Flux uses a low-solids no-clean liquid formulation without halides, rosin, or resin for foam and wave soldering. It is designed for fast wetting and leaves a very small amount of barely visible, tack-free, noncorrosive residue. This residue profile supports accurate pin testing and eliminates a required post-solder cleaning step under the documented use conditions. The flux is classified ORL0 under IPC J-STD-004 and L3NC under IPC-SF-818. As supplied, it contains 2.1% solids, has an 11 deg C flash point, and carries a 540-day shelf life. Typical specific gravity is 0.812 +/- 0.005 at 25 deg C; acid number is 16.5 +/- 1.0 mg KOH/g.

Key features

  • Halide- and rosin-free: Low-solids formulation supports no-clean electronics soldering.
  • Fast wetting: Designed for efficient foam and wave soldering application.
  • Tack-free noncorrosive residue: Barely visible residue supports accurate pin testing without required cleaning.

Applications

Foam or wave soldering for electronic circuit assemblies.

Product Family

ALPHA SM351F

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Solids
2.1 %
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
0.812 ± 0.005 @25°C

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
AppearanceClear, pale-yellow liquidTypical
Solids content2.1% by weightTypical
Specific gravity0.812 +/- 0.00525 deg C
Acid number16.5 +/- 1.0mg KOH/gTypical
Flash point11deg CT.C.C.
Shelf life540daysFrom date of manufacture
Flux classificationORL0IPC J-STD-004