ALPHA SLS65C

Harmonization Code : 3404.90.00.00 | Artificial waxes and prepared waxes : Other

ALPHA SLS65C

Main features

  • Low-solids, no-clean flux formulated to reduce solder balling and solder bridging in wave and chip-wave soldering.
  • Very low level of non-tacky residue supports pin testing while allowing residues to remain on the board without cleaning.
  • Supports foam, wave, and spray application methods with documented Bellcore and IPC electrical test performance.

Product Description

ALPHA SLS 65C No-Clean Flux is an active, low-solids liquid flux developed for wave soldering applications where solder balling, solder bridging, and residue can affect assembly quality and inspection. The standard formulation contains 2.2% solids and uses organic activators with additives designed to reduce surface tension between the solder mask and solder. Its thermally stable formulation is designed to reduce solder bridging, while the very low level of non-tacky residue supports pin testing without requiring post-solder cleaning. ALPHA SLS 65C can be applied by foam, wave, or spray methods and carries an ORL0 designation according to IPC J-STD-004.

Key features

  • Reduced solder balling and bridging: Formulated to reduce surface tension between solder mask and solder and improve thermal stability during wave soldering.
  • Low-solids, no-clean formulation: Contains 2.2% solids with a very low level of non-tacky residue designed to remain on the board without cleaning.
  • Flexible flux application: Suitable for foam, wave, and spray application methods.

Applications / Suitable for

  • Wave soldering and chip-wave processes
  • Assemblies sensitive to solder bridging and solder balling
  • Assemblies requiring pin testing with minimal flux residue
Product Family

ALPHA SLS65C

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Solids
2.2 %
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
0.799 ± 0.003 @25°C

Additional Information

Technical properties

As-supplied / before-processing properties

Selected typical properties of ALPHA SLS 65C in its as-supplied liquid state.

Property Value Unit Method or condition
Appearance Clear, colorless liquid - As supplied
Solids content 2.2 wt/wt % Typical value
Acid number 18 mg KOH/g Typical value
Specific gravity 0.799 +/- 0.003 - 25 °C (77 °F)
pH 3.4 - 5% aqueous solution
Flash point 53 (12) °F (°C) TCC
Technical properties

After-processing / final-state properties

Selected corrosion and electrical test results for ALPHA SLS 65C under the stated test conditions.

Property Value Unit Method or condition
Surface insulation resistance - Comb-Down 8.8 x 1012 ohms Bellcore GR78-CORE, Issue 1; uncleaned; 35 °C/85% RH, 5 days, -48 V
Surface insulation resistance - Comb-Up 1.4 x 1012 ohms Bellcore GR78-CORE, Issue 1; uncleaned; 35 °C/85% RH, 5 days, -48 V
IPC SIR - Comb-Down 5.6 x 109 ohms IPC J-STD-004; uncleaned; 85 °C/85% RH, 7 days, -50 V
IPC SIR - Comb-Up 2.3 x 109 ohms IPC J-STD-004; uncleaned; 85 °C/85% RH, 7 days, -50 V
Electromigration Pass - Bellcore GR78-CORE, Issue 1; uncleaned; 65 °C/85% RH, 500 hours, 10 V