ALPHA SLS65

Harmonization Code : 3404.90.00.00 | Artificial waxes and prepared waxes : Other

ALPHA SLS65

Main features

  • Thermally Stable Bridge Control
  • Low Solder-Ball Tendency
  • Foam, Wave, or Spray Application

Product Description

ALPHA SLS 65 Liquid Soldering Flux provides an active, low-solids no-clean liquid formulation for wave soldering by foam, wave, or spray application. Its thermally stable activator system is designed to reduce solder bridging, while surface-tension control lowers solder-ball formation across a range of solder masks. The formulation leaves very low, non-tacky residue to limit interference with pin testing and maintain clean board appearance. The ready-to-use liquid contains 2.3% solids and is classified ORL0 under IPC J-STD-004. At 25 deg C, typical specific gravity is 0.801 +/- 0.003; acid number is 18 +/- 1 mg KOH/g. Application settings should be optimized for the board, components, and equipment.

Key features

  • Thermally stable activation: Designed to reduce solder bridging in low-solids no-clean processing.
  • Solder-ball control: Reduced surface tension limits solder-ball formation across varied solder masks.
  • Low non-tacky residue: Very low residue supports pin testing and clean board appearance.

Applications

Wave soldering using foam, wave, or spray flux application.

Product Family

ALPHA SLS65

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Solids
2.3 %
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
0.801 ± 0.003 @25°C

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
AppearanceClear, colorless liquidTypical
Solids content2.3% by weightTypical
Specific gravity0.801 +/- 0.00325 deg C +/- 1.8 deg C
Acid number18 +/- 1mg KOH/gTypical
pH3.36 +/- 0.305% aqueous solution
Flash point12deg CT.C.C.
Shelf life360daysFrom date of manufacture
Flux classificationORL0IPC J-STD-004