ALPHA NR200

Harmonization Code : 3404.90.00.00 | Artificial waxes and prepared waxes : Other

ALPHA NR200

Main features

  • Low-Residue Pin-Test Surface
  • Foam, Spray, or Wave Fluxing
  • High-SIR Tack-Free Surface

Product Description

ALPHA NR200 Liquid Soldering Flux uses a ready-to-use, halide-free, rosin- and resin-free, low-solids formulation for wave soldering through-hole, mixed-technology, and surface-mount assemblies. It can be applied by foam, spray, or wave methods and combines high activity with virtually no visible residue on most solder masks. The resulting surface is tack-free and supports accurate pin testing without a separate cleaning step. Enhanced foaming and low odor add process flexibility. Typical as-supplied data include 2.0% solids, 0.805 +/- 0.003 specific gravity at 25 deg C, an ORM0 designation, and a 14 deg C T.C.C. flash point.

Key Features

  • Low visible residue: Virtually no visible residue on most solder masks after wave soldering.
  • Multiple application methods: Ready for foam, spray, or wave flux application.
  • Pin-testable surface: Tack-free surface supports accurate pin testing without a separate cleaning step.

Applications

Wave soldering of through-hole, mixed-technology, and surface-mount assemblies using foam, spray, or wave application.

Product Family

ALPHA NR200

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Solids
7.0 %
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
0.798 ± 0.005 @25°C

Additional Information

Typical Properties

As Supplied

Typical values for the ready-to-use liquid flux.

PropertyTypical ValueUnitsMethod or Condition
AppearanceClear, colorless liquidVisual
Solids content2.0% by weightTypical
Specific gravity0.805 +/- 0.00325 deg C
Acid number18 +/- 1mg KOH/gTypical
Flash point14deg CT.C.C.
Shelf life540daysTypical
Flux classificationORM0J-STD-004