ALPHA EF6000

Harmonization Code : 3404.90.00.00 | Artificial waxes and prepared waxes : Other

ALPHA EF6000

Main features

  • Low-Residue Rosin-Free No-Clean Flux
  • Broad Lead-Free and Tin-Lead Window
  • Reduced Solder-Ball and Bridging Tendency

Product Description

ALPHA EF-6000 Liquid Soldering Flux is an active, rosin-free, low-solids, low-residue no-clean alcohol-based flux for lead-free and tin-lead wave and selective soldering. Typical solids content is 2.2%, supporting minimal residue and pin testability after soldering. The formulation has a broad thermal process window and is designed to maintain hole fill across varying preheat temperatures and dwell times. Additives reduce the tendency for solder balling, while the thermally stable formulation helps reduce bridging during dual-wave processing. The product is classified ORL0 under IPC J-STD-004 and is supplied as a clear to pale-yellow liquid.

Key features

  • Rosin-free low-residue chemistry: A 2.2% solids no-clean formulation minimizes deposited residue and supports pin-test access after soldering.
  • Broad thermal process window: Supports lead-free and tin-lead wave or selective soldering across varying preheat temperatures and dwell times.
  • Solder ball and bridging control: The formulation is designed to reduce solder-ball generation and bridging during wave and selective soldering.

Applications

Used for lead-free and tin-lead wave or selective soldering of assemblies that require low residue, pin testability, and a broad process window.

Product Family

ALPHA EF6000

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Solids
2.2 %
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
0.790 ± 0.003 @25°C

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
AppearanceClear to pale-yellow liquidAs supplied
Solids content2.2%Typical
Specific gravity0.790 +/- 0.003At 25 deg C
Acid number17.5 +/- 1mg KOH/gTypical
pH3.35% aqueous solution
Flash point12deg CTypical
Shelf life360daysFrom date of manufacture
IPC classificationORL0IPC J-STD-004

Leading Brands Trust in Our Products and Services