ALPHA EF-9301

Harmonization Code : 3404.90.00.00 | Artificial waxes and prepared waxes : Other

ALPHA EF-9301

Main features

  • Greater Than 95% Hole Fill
  • Low-Bridging SMT Soldering
  • Spray or Foam Fluxing

Product Description

ALPHA EF-9301 Liquid Soldering Flux is a rosin-containing, ready-to-use liquid flux developed for full-dulling wave soldering with tin-lead and lead-free alloys. Spray or foam application produces smooth, dull solder joints with evenly spread, low-tack residue. On connectors and bottom-side SMT components, the flux shows low bridging together with strong hole fill and low solder balling. Hole-fill yield is greater than 95% on 10 mil holes. The typical solids level is 7.0%, with specific gravity of 0.798 +/- 0.005 at 25 deg C and ROM1 classification. Separate process recommendations cover preheat and solder-pot temperatures for tin-lead and lead-free operation.

Key Features

  • High hole-fill yield: Greater than 95% hole-fill yield on 10 mil holes.
  • Low-bridging soldering: Low bridging on connectors and bottom-side SMT components.
  • Flexible flux application: Ready for spray or foam application in tin-lead and lead-free processes.

Applications

Wave soldering with tin-lead and lead-free alloys using spray or foam flux application.

Product Family

ALPHA EF-9301

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Solids
7.0 %
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
0.798 ± 0.005 @25°C

Additional Information

Typical Properties

As Supplied

Typical values for the ready-to-use liquid flux.

PropertyTypical ValueUnitsMethod or Condition
AppearanceClear, pale yellow liquidVisual
Solids content7.0% by weightTypical
Specific gravity0.798 +/- 0.00525 deg C
Acid number16 to 17mg KOH/gTypical
pH3.6Typical
Flash point12deg CT.C.C.
Shelf life360daysTypical
Flux classificationROM1J-STD-004