ALPHA EF-2210

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

ALPHA EF-2210

Main features

  • Low-Solids Residue for Legacy Processing
  • OSP Wave and Selective Soldering
  • Defined EF-2100 Replacement Path

Product Description

ALPHA EF-2210 Liquid Soldering Flux has been discontinued. It is a legacy VOC-free, halide-free, rosin/resin-free, 4% solids no-clean flux for wave and selective soldering. The historical process scope includes both tin-lead and lead-free soldering and OSP-coated bare copper boards that have experienced prior thermal excursions. Residues are designed to remain on the board and can be removed with hot water when cleaning is needed. For rotary-drum spray fluxing, DI water is the thinner and the acid number is controlled to 28.5 to 33.5. MacDermid Alpha identifies ALPHA EF-2100 as the direct replacement for EF-2210.

Key features

  • VOC-free low-solids chemistry: A 4% solids, halide-free, rosin/resin-free no-clean formulation supports low-residue legacy wave and selective soldering.
  • OSP and dual-alloy process fit: Historical guidance covers OSP-coated bare copper boards plus tin-lead and lead-free soldering conditions.
  • Direct EF-2100 replacement: MacDermid Alpha identifies ALPHA EF-2100 as the direct replacement for current product selection.

Applications

Historical applications include wave and selective soldering of electronic assemblies, including OSP-coated bare copper boards, under the established EF-2210 process conditions.

Product Family

ALPHA EF-2210

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Solids
4.0 %
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.015 ± 0.003 @25°C

Additional Information

Technical properties

As-supplied / before-processing properties

Values apply to the discontinued EF-2210 grade.

PropertyValueUnitMethod / condition
AppearanceClear, colorless liquidTypical
Solids content4.0% by weightTypical
Specific gravity1.015 +/- 0.003At 25 deg C (77 deg F)
Acid number31.5 +/- 2.0mg KOH/gTypical
VOC content< 1%Typical
Flash pointNoneT.C.C.
Shelf life18monthsTypical
IPC classificationORL0IPC J-STD-004

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers