ALPHA CVP 520

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

ALPHA CVP 520

Main features

  • Low-Temperature Reflow for Sensitive Assemblies
  • Extended Eight-Hour Stencil Life
  • Configurable Alloy and Powder Selection

Product Description

ALPHA CVP-520 Solder Paste is a configurable low-temperature, lead-free, no-clean solder paste family for surface-mount assembly. Available Sn/Bi/Ag and Sn/Bi alloy options have melting points below 140 deg C and have been used with peak reflow profiles of 155 to 190 deg C. Type 3, Type 4, and Type 5 powder sizes are available by configuration, and the paste supports standard and fine-pitch stencil printing. Stencil life exceeds eight hours at 23 deg C and 50% RH. After reflow, the flux residue is clear and colorless and is designed to remain on the board. Exact alloy, powder size, and package are selected by SKU.

Key features

  • Low-temperature reflow: Alloy options melt below 140 deg C and support peak reflow profiles of 155 to 190 deg C for temperature-sensitive assembly work.
  • Extended stencil life: A stencil life greater than eight hours at 23 deg C and 50% RH supports sustained printing operations.
  • Configurable printing formats: Type 3, Type 4, and Type 5 powders and multiple alloy options let the selected SKU match standard or fine-pitch printing needs.

Applications

Used for low-temperature SMT assembly, repeated-reflow processes with temperature-sensitive components or connectors, and supported BGA or through-hole integration using the selected configuration.

Product Family

ALPHA CVP 520

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Alloy Composition
Composition of the alloy material
Sn42/Bi57.6/Ag0.4; Sn42/Bi57/Ag1.0; Sn42/Bi58

Additional Information

Technical properties

As-supplied / before-processing properties

Values and options apply to the CVP-520 family; exact alloy, powder type, and package are selected by SKU.

PropertyValueUnitMethod / condition
Available alloys42% Sn / 57.6% Bi / 0.4% Ag; 42% Sn / 57% Bi / 1.0% Ag; 42% Sn / 58% Bi1.0% Ag alloy available on request
Powder sizeType 3, Type 4, Type 5Available family configurations
Residue content~5% by weightApproximate
Stencil life>8hoursAt 23 deg C and 50% RH
Refrigerated storage0 to 10deg CFor guaranteed stability
Refrigerated shelf life6monthsRefrigerated paste
Room-temperature storage2weeksUp to 25 deg C before use
Technical properties

After-processing / final-state properties

Results apply to the selected CVP-520 configuration and the stated test conditions.

PropertyValueUnitMethod / condition
Flux residue appearanceClear, colorlessAfter reflow
Surface insulation resistancePass; >= 1 x 10^8ohmIPC J-STD-004C / TM-650 2.6.3.7; 7 days at 85 deg C / 85% RH, 12 V
ElectromigrationPass; final > 1 x 10^10ohmJIS Z 3197:1999; 1000 hours at 85 deg C / 85% RH, 48 V DC; no migration
Voiding classificationClass 3IPC-7095; obtained with the stated reflow profile

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers