ALPHA AutoClean 40 Electronic Cleaner

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

ALPHA AutoClean 40 Electronic Cleaner

Main features

  • Ready-to-Use Aqueous Cleaning
  • Immersion, Ultrasonic, or Manual Cleaning
  • Non-Flammable Water-Based Formulation

Product Description

ALPHA® AutoClean 40 Electronic Cleaner is a water-based aqueous cleaning fluid formulated for the removal of pre- and post-soldering flux residues from electronic assemblies and production equipment. Designed for use at full strength, it combines surfactants and emulsifiers to clean dissolved soils while helping inhibit their redeposition. The cleaner is effective at ambient temperature and can be used in immersion, agitation, ultrasonic, or manual-wipe processes.

Key Features

  • Ready-to-use aqueous cleaner: Used as received at 100% concentration without dilution.
  • Effective flux-residue removal: Removes high-rosin flux residues from printed circuit assemblies, flux equipment, ovens, pallets, carriers, and jigs.
  • Flexible cleaning methods: Suitable for immersion with agitation, soaking, ultrasonic cleaning, and manual wiping at ambient temperature to 38°C (100°F).
  • Non-flammable formulation: Contains no CFCs or chlorinated solvents and has no flash point below boiling.

Applications / Suitable for

  • Removal of pre- and post-soldering flux residues from printed circuit assemblies
  • Cleaning flux spray equipment, ovens, selective-soldering pallets, carriers, and jigs
  • Immersion, agitation, soak, ultrasonic, and manual-wipe cleaning processes

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
clear colorless liquid
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1
Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
none to boiling °C

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Typical physical and storage properties of the supplied electronic cleaner.

Property Value Unit Method / Condition
Appearance Clear, colorless liquid — May become cloudy when stored above 25°C (77°F); shake thoroughly before use
Specific Gravity 1.0 — At 20°C
pH <12 — As supplied
Flash Point None to boiling °F Non-flammable aqueous formulation
Use Concentration 100 % Use as received
Shelf Life 1080 days Unopened containers stored in a cool, dry location at 5 to 30°C