ALPHA 90IA

Harmonization Code : 3404.90.00.00 | Artificial waxes and prepared waxes : Other

ALPHA 90IA

Main features

  • High-Activity Difficult-Metal Soldering
  • Low-Temperature Light-Gauge Processing
  • Defined Acid-Wash Residue Removal

Product Description

ALPHA 90 Water Soluble Inorganic Acid Flux is a strong, highly active liquid flux for stainless steel and other difficult-to-solder metals. Its low activation temperature is suited to light-gauge materials where excessive heat can cause buckling or discoloration. Wetting agents promote rapid, uniform penetration into joint areas, while the active fluxing system reduces spattering. The flux is used for dip soldering and can be heated by torch, iron, oven, resistance, or induction methods. Post-solder residues are corrosive and must be removed promptly with a 1% hydrochloric acid solution followed by a water rinse. Typical specific gravity is 1.32 +/- 0.01 at 25 deg C.

Key features

  • High-activity difficult-metal soldering: Designed for stainless steel and other difficult-to-solder metals that need strong inorganic-acid activation.
  • Low-temperature activation: Supports light-gauge soldering where lower heat input helps limit buckling or discoloration.
  • Defined residue removal: Corrosive post-solder residues are removed with a 1% hydrochloric acid wash followed by a water rinse.

Applications

Used for dip soldering of cans, hardware, and similar articles with torch, iron, oven, resistance, or induction heating across the listed difficult-to-solder metals.

Product Family

ALPHA 90IA

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.32 ± 0.01* @25°C

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
AppearanceYellow to amber liquidTypical
Specific gravity1.32 +/- 0.01At 25 deg C (77 deg F)
Weight per gallon11.0lb/galAt 25 deg C (77 deg F)
Flash pointNone
Shelf life1080daysFrom date of manufacture