ALPHA 611F

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

ALPHA 611F

Main features

  • Low-Pressure Fine-Foam Control
  • Stable Continuous-Aeration Performance
  • Defined Daily Flux Maintenance

Product Description

ALPHA 611F RMA Flux is an amber, mildly activated rosin liquid flux formulated for fine-bubble foam application. It develops a constant, adjustable foam head at low air pressure and maintains foaming, fluxing, and wetting behavior during continuous aeration. Its 37% solids content supports coverage on dense plated-through-hole circuit boards. Maintain the foam system by controlling air pressure, keeping moisture and oil out of the air lines, and adjusting specific gravity with the proper thinner at least daily. Flux replacement after 40 hours of use provides a defined operating interval for the foam process.

Key features

  • Fine foam at low pressure: A constant, adjustable fine-bubble head supports controlled coverage without high air pressure.
  • Stable during continuous aeration: Foaming, fluxing, and wetting behavior remain consistent during ongoing foam-system operation.
  • Defined foam-process control: Daily specific-gravity adjustment and a 40-hour replacement interval support repeatable flux management.

Applications

Applications include fine-bubble foam fluxing for dense plated-through-hole circuit boards and other supported RMA soldering processes.

Product Family

ALPHA 611F

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Solids
37 %
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
0.918 ± 0.005 @25°C

Additional Information

Technical properties

As-supplied / before-processing properties

Maintain specific gravity with the proper thinner and replace the working flux after 40 hours of use.

PropertyValueUnitMethod / condition
AppearanceAmber liquidAs supplied
Solids content37%Typical
Specific gravity0.918 +/- 0.00525 deg C
Weight per gallon7.64lb/gal25 deg C
Flash point18deg CT.C.C.
Water-extract resistivity260,000ohm cmTypical
Shelf life540daysFrom date of manufacture